| Category | Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS) |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | Noryl |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | SABIC Innovative Plastics NORYL PX1712 PPE+HIPS (Asia Pacific).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.07 g/cc | 1.07 g/cc | ASTM D792 |
| Water Absorption | 0.030 % <br>@Time 86400 sec |
0.030 % <br>@Time 24.0 hour |
ASTM D570 |
| Linear Mold Shrinkage, Flow | 0.0050 - 0.0070 cm/cm <br>@Thickness 3.20 mm |
0.0050 - 0.0070 in/in <br>@Thickness 0.126 in |
SABIC Method |
| Melt Flow | 6.9 g/10 min <br>@Load 5.00 kg,<br> Temperature 300 °C |
6.9 g/10 min <br>@Load 11.0 lb,<br> Temperature 572 °F |
ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 124 | 124 | ASTM D785 |
| Tensile Strength, Yield | 71.0 MPa | 10300 psi | SABIC - Japan Method |
| Elongation at Break | 50 % | 50 % | SABIC - Japan Method |
| Flexural Strength | 98.0 MPa | 14200 psi | ASTM D790 |
| Flexural Modulus | 2.45 GPa | 355 ksi | ASTM D790 |
| Izod Impact, Notched | 1.11 J/cm | 2.08 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 60.0 µm/m-°C <br>@Temperature -30.0 - 30.0 °C |
33.3 µin/in-°F <br>@Temperature -22.0 - 86.0 °F |
TMA |
| Deflection Temperature at 1.8 MPa (264 psi) | 148 °C <br>@Thickness 6.40 mm |
298 °F <br>@Thickness 0.252 in |
unannealed; ASTM D648 |