Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.18 g/cc | 1.18 g/cc | ASTM D792 |
Density | 1.19 g/cc | 0.0430 lb/in³ | ISO 1183 |
Moisture Absorption | 0.150 % | 0.150 % | 23°C / 50% RH; ISO 62 |
Water Absorption at Saturation | 0.35 % | 0.35 % | ISO 62 |
Linear Mold Shrinkage, Flow | 0.0040 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
Melt Flow | 10 g/10 min @Load 1.20 kg, Temperature 300 °C |
10 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Melt Index of Compound | 9.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 50.0 MPa | 7250 psi | Type I, 50 mm/min; ASTM D638 |
60.0 MPa | 8700 psi | 50 mm/min; ISO 527 | |
Tensile Strength, Yield | 56.0 MPa | 8120 psi | Type I, 50 mm/min; ASTM D638 |
57.0 MPa | 8270 psi | 50 mm/min; ISO 527 | |
Elongation at Break | 98 % | 98 % | Type I, 50 mm/min; ASTM D638 |
120 % | 120 % | 50 mm/min; ISO 527 | |
Elongation at Yield | 6.0 % | 6.0 % | 50 mm/min; ISO 527 |
6.0 % | 6.0 % | Type I, 50 mm/min; ASTM D638 | |
Tensile Modulus | 2.02 GPa | 293 ksi | 50 mm/min; ASTM D638 |
2.15 GPa | 312 ksi | 1 mm/min; ISO 527 | |
Flexural Yield Strength | 85.0 MPa | 12300 psi | 2 mm/min; ISO 178 |
92.0 MPa | 13300 psi | 1.3 mm/min, 50 mm span; ASTM D790 | |
Flexural Modulus | 2.23 GPa | 323 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
2.25 GPa | 326 ksi | 2 mm/min; ISO 178 | |
Izod Impact, Notched | 8.65 J/cm | 16.2 ft-lb/in | ASTM D256 |
7.74 J/cm @Temperature -30.0 °C |
14.5 ft-lb/in @Temperature -22.0 °F |
ASTM D256 | |
Izod Impact, Notched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80*10*3; ISO 180/1A |
60.0 kJ/m² @Temperature -30.0 °C |
28.6 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A | |
Izod Impact, Unnotched (ISO) | NB | NB | 80*10*3; ISO 180/1U |
NB @Temperature -30.0 °C |
NB @Temperature -22.0 °F |
80*10*3; ISO 180/1U | |
Charpy Impact Unnotched | NB | NB | Edgew 80*10*3 sp=62mm; ISO 179/1eU |
NB @Temperature -30.0 °C |
NB @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eU | |
Charpy Impact, Notched | 7.00 J/cm² | 33.3 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
6.50 J/cm² @Temperature -30.0 °C |
30.9 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA | |
Dart Drop, Total Energy | 70.0 J @Temperature 23.0 °C |
51.6 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
77.0 J @Temperature -30.0 °C |
56.8 ft-lb @Temperature -22.0 °F |
ASTM D3763 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.9 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
72.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
40.0 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 | |
CTE, linear, Transverse to Flow | 70.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.9 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
72.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
40.0 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 | |
Deflection Temperature at 0.46 MPa (66 psi) | 140 °C | 284 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
139 °C @Thickness 3.20 mm |
282 °F @Thickness 0.126 in |
unannealed; ASTM D648 | |
Deflection Temperature at 1.8 MPa (264 psi) | 128 °C | 262 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
124 °C @Thickness 3.20 mm |
255 °F @Thickness 0.126 in |
unannealed; ASTM D648 | |
Vicat Softening Point | 145 °C | 293 °F | Rate B/50; ASTM D1525 |
145 °C | 293 °F | Rate B/50; ISO 306 | |
146 °C | 295 °F | Rate B/120; ISO 306 |
Descriptive Properties | Value | Comments |
---|---|---|
Ball Pressure Test, 125°C +/- 2°C | PASSES | IEC 60695-10-2 |