Network Polymers NPP 50-0158

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer Network Polymers
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Network Polymers NPP 50-0158.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: High Density Polyethylene (HDPE)Information provided by Network Polymers Inc.
Physical Properties Metric English Comments
Density 0.958 g/cc
0.0346 lb/in³
ASTM D1505
ESCR 100% Igepal® 20 hour
20 hour
Condition A; ASTM D1693
High Load Melt Index 0.96 g/10 min

@Load 21.6 kg,
Temperature 190 °C
0.96 g/10 min

@Load 47.6 lb,
Temperature 374 °F
Procedure A Condition F (HLMI); ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 67
67
ASTM D2240
Tensile Strength, Yield 27.6 MPa
4000 psi
2 in per min; ASTM D638
Elongation at Break 1200 %
1200 %
Flexural Modulus 1.10 GPa
160 ksi
ASTM D790
Thermal Properties Metric English Comments
Brittleness Temperature <= -70.6 °C
<= -95.0 °F
ASTM D746