| Category | Polymer , Thermoplastic , Nylon , Nylon 6 |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | LNP Konduit |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | SABIC Innovative Plastics LNP KONDUIT PX08322 PA 6 (Europe-Africa-Middle East).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.52 g/cc | 0.0549 lb/in³ | ISO 1183 |
| Water Absorption | 0.39 % <br>@Time 86400 sec |
0.39 % <br>@Time 24.0 hour |
SABIC Method |
| Moisture Absorption | 0.0600 % | 0.0600 % | 23°C / 50% RH; ISO 62 |
| Linear Mold Shrinkage, Flow | 0.0024 cm/cm <br>@Time 86400 sec |
0.0024 in/in <br>@Time 24.0 hour |
ISO 294 |
| Linear Mold Shrinkage, Transverse | 0.0028 cm/cm <br>@Time 86400 sec |
0.0028 in/in <br>@Time 24.0 hour |
ISO 294 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 45.0 MPa | 6530 psi | 5 mm/min; ISO 527 |
| Elongation at Break | 0.60 % | 0.60 % | 5 mm/min; ISO 527 |
| Tensile Modulus | 11.0 GPa | 1600 ksi | 1 mm/min; ISO 527 |
| Flexural Strength | 76.0 MPa | 11000 psi | 2 mm/min; ISO 178 |
| Flexural Modulus | 11.3 GPa | 1640 ksi | 2 mm/min; ISO 178 |
| Izod Impact, Notched (ISO) | 2.00 kJ/m² | 0.952 ft-lb/in² | 80*10*4; ISO 180/1A |
| Izod Impact, Unnotched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | 80*10*4; ISO 180/1U |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 25.3 µm/m-°C <br>@Temperature -30.0 - 80.0 °C |
14.1 µin/in-°F <br>@Temperature -22.0 - 176 °F |
ISO 11359-2 |
| 29.9 µm/m-°C <br>@Temperature 23.0 - 80.0 °C |
16.6 µin/in-°F <br>@Temperature 73.4 - 176 °F |
ISO 11359-2 | |
| CTE, linear, Transverse to Flow | 51.4 µm/m-°C <br>@Temperature -30.0 - 80.0 °C |
28.6 µin/in-°F <br>@Temperature -22.0 - 176 °F |
ISO 11359-2 |
| 61.7 µm/m-°C <br>@Temperature 23.0 - 80.0 °C |
34.3 µin/in-°F <br>@Temperature 73.4 - 176 °F |
ISO 11359-2 | |
| Thermal Conductivity | 0.920 W/m-K | 6.38 BTU-in/hr-ft²-°F | through-plane, ø80*3mm discs; ISO 22007-2 |
| 2.10 W/m-K | 14.6 BTU-in/hr-ft²-°F | through-plane, 10*10*3mm sample; ASTM E 1461-07 | |
| 5.09 W/m-K | 35.3 BTU-in/hr-ft²-°F | in-plane, ø80*3mm discs; ISO 22007-2 | |
| 8.10 W/m-K | 56.2 BTU-in/hr-ft²-°F | in-plane, ø25*0.4mm disc; ASTM E 1461-07 | |
| Deflection Temperature at 1.8 MPa (264 psi) | 165 °C | 329 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
| Flammability, UL94 | V-0 <br>@Thickness 1.20 mm |
V-0 <br>@Thickness 0.0472 in |
UL 94 |
| Glow Wire Test | 825 °C | 1520 °F | IEC 60695-2-13 |
| 960 °C <br>@Thickness 1.00 mm |
1760 °F <br>@Thickness 0.0394 in |
IEC 60695-2-12 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Surface Resistance | >= 1.00e+15 ohm | >= 1.00e+15 ohm | ASTM D257 |
| Dielectric Constant | 4.8 <br>@Frequency 1.00e+6 Hz |
4.8 <br>@Frequency 1.00e+6 Hz |
ASTM D150 |
| 7.27 <br>@Frequency 50.0 - 60.0 Hz |
7.27 <br>@Frequency 50.0 - 60.0 Hz |
ASTM D150 | |
| Dielectric Strength | 14.1 kV/mm <br>@Thickness 1.00 mm |
358 kV/in <br>@Thickness 0.0394 in |
in oil; ASTM D149 |
| Dissipation Factor | 0.043 <br>@Frequency 1.00e+6 Hz |
0.043 <br>@Frequency 1.00e+6 Hz |
ASTM D150 |
| 0.083 <br>@Frequency 50.0 - 60.0 Hz |
0.083 <br>@Frequency 50.0 - 60.0 Hz |
ASTM D150 | |
| Comparative Tracking Index | 575 V | 575 V | IEC 60112 |
| Hot Wire Ignition, HWI | >= 120 sec | >= 120 sec | UL 746A |
| High Amp Arc Ignition, HAI | >= 120 arcs | >= 120 arcs | UL 746A |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Ball Pressure Test, 125°C +/- 2°C | PASSES | IEC 60695-10-2 |
| Water Immersion, Start F1 from 1mm onward | PASSES | UL 746C |
| PASSES | UL 746C |