Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BYK Cloisite® 20A Nanoclay

Category Other Engineering Material , Additive/Filler for Polymer , Polymer
Manufacturer BYK Additives
Trade Name Cloisite®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BYK Cloisite® 20A Nanoclay.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Cloisite® 20A is an additive for plastics to improve various plastic physical properties, such as reinforcement, HDT, CLTE and barrier.Information provided by Southern Clay ProductsSouthern Clay Products is now a part of BYK Additives.
Physical Properties Metric English Comments
Specific Gravity 1.77 g/cc
1.77 g/cc
Bulk Density 0.118 g/cc
0.00425 lb/in³
Loose
0.2171 g/cc
0.007841 lb/in³
Packed
Loss On Ignition 38 %
38 %
Particle Size <= 2.0 µm
<= 2.0 µm
10%
<= 6.0 µm
<= 6.0 µm
50%
<= 13 µm
<= 13 µm
90%
Mechanical Properties Metric English Comments
Hardness, Shore D 83
83
5% Cloisite® reinforced Nylon 6
Tensile Strength, Ultimate 101 MPa
14600 psi
5% Cloisite® reinforced Nylon 6
Elongation at Break 8.0 %
8.0 %
5% Cloisite® reinforced Nylon 6
Modulus of Elasticity 4.657 GPa
675.5 ksi
5% Cloisite® reinforced Nylon 6
Flexural Modulus 3.78 GPa
548 ksi
5% Cloisite® reinforced Nylon 6
Izod Impact, Notched 0.270 J/cm
0.506 ft-lb/in
5% Cloisite® reinforced Nylon 6
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 96.0 °C
205 °F
5% Cloisite® reinforced Nylon 6
Processing Properties Metric English Comments
Moisture Content <= 2.0 %
<= 2.0 %
Descriptive Properties Value Comments
Modifier Concentration, meq/ 100g clay 95
Organic Modifier dimethyl, dihydrogenated tallow, quaternary ammonium
X-Ray Diffraction d-Spacing (001) 31.5 Angstroms