| Category | Polymer , Thermoplastic , ASA Polymer , Polycarbonate (PC) , Polycarbonate/ASA Alloy, Unreinforced |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | GELOY |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | SABIC Innovative Plastics GELOY HRA222 ASA+PC (Europe-Africa-Middle East).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.17 g/cc | 0.0423 lb/in³ | ISO 1183 |
| Moisture Absorption | 0.200 % | 0.200 % | 23°C / 50% RH; ISO 62 |
| Water Absorption at Saturation | 0.60 % | 0.60 % | ISO 62 |
| Linear Mold Shrinkage, Flow | 0.0040 - 0.0060 cm/cm | 0.0040 - 0.0060 in/in | on Tensile Bar; SABIC Method |
| Melt Index of Compound | 13 g/10 min <br>@Load 2.16 kg,<br> Temperature 260 °C |
13 g/10 min <br>@Load 4.76 lb,<br> Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 45.0 MPa | 6530 psi | 50 mm/min; ISO 527 |
| 51.0 MPa | 7400 psi | 5 mm/min; ISO 527 | |
| 56.0 MPa | 8120 psi | Type I, 50 mm/min; ASTM D638 | |
| 66.0 MPa | 9570 psi | Type I, 5 mm/min; ASTM D638 | |
| Tensile Strength, Yield | 59.0 MPa | 8560 psi | Type I, 5 mm/min; ASTM D638 |
| 60.0 MPa | 8700 psi | 50 mm/min; ISO 527 | |
| 62.0 MPa | 8990 psi | 5 mm/min; ISO 527 | |
| 63.0 MPa | 9140 psi | Type I, 50 mm/min; ASTM D638 | |
| Elongation at Break | >= 50 % | >= 50 % | 5 mm/min; ISO 527 |
| >= 50 % | >= 50 % | 50 mm/min; ISO 527 | |
| >= 100 % | >= 100 % | Type I, 50 mm/min; ASTM D638 | |
| >= 100 % | >= 100 % | Type I, 5 mm/min; ASTM D638 | |
| Elongation at Yield | 4.2 % | 4.2 % | Type I, 5 mm/min; ASTM D638 |
| 4.3 % | 4.3 % | 5 mm/min; ISO 527 | |
| 4.3 % | 4.3 % | Type I, 50 mm/min; ASTM D638 | |
| 4.4 % | 4.4 % | 50 mm/min; ISO 527 | |
| Tensile Modulus | 2.52 GPa | 365 ksi | 1 mm/min; ISO 527 |
| 2.59 GPa | 376 ksi | 5 mm/min; ASTM D638 | |
| Flexural Yield Strength | 93.0 MPa | 13500 psi | 2 mm/min; ISO 178 |
| Flexural Modulus | 2.51 GPa | 364 ksi | 2 mm/min; ISO 178 |
| Izod Impact, Notched | 3.85 J/cm | 7.21 ft-lb/in | ASTM D256 |
| 2.90 J/cm <br>@Temperature 0.000 °C |
5.43 ft-lb/in <br>@Temperature 32.0 °F |
ASTM D256 | |
| Izod Impact, Notched (ISO) | 17.0 kJ/m² | 8.09 ft-lb/in² | 80*10*4; ISO 180/1A |
| 9.00 kJ/m² <br>@Temperature -30.0 °C |
4.28 ft-lb/in² <br>@Temperature -22.0 °F |
80*10*4; ISO 180/1A | |
| 12.0 kJ/m² <br>@Temperature 0.000 °C |
5.71 ft-lb/in² <br>@Temperature 32.0 °F |
80*10*4; ISO 180/1A | |
| Charpy Impact, Notched | 1.50 J/cm² | 7.14 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 69.0 µm/m-°C <br>@Temperature -30.0 - 80.0 °C |
38.3 µin/in-°F <br>@Temperature -22.0 - 176 °F |
ISO 11359-2 |
| CTE, linear, Transverse to Flow | 71.0 µm/m-°C <br>@Temperature -30.0 - 80.0 °C |
39.4 µin/in-°F <br>@Temperature -22.0 - 176 °F |
ISO 11359-2 |
| 75.0 µm/m-°C <br>@Temperature 23.0 - 80.0 °C |
41.7 µin/in-°F <br>@Temperature 73.4 - 176 °F |
ISO 11359-2 | |
| Deflection Temperature at 0.46 MPa (66 psi) | 99.0 °C | 210 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
| Deflection Temperature at 1.8 MPa (264 psi) | 88.0 °C | 190 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
| Vicat Softening Point | 102 °C | 216 °F | Rate B/50; ISO 306 |
| 104 °C | 219 °F | Rate B/120; ISO 306 | |
| 111 °C | 232 °F | Rate A/50; ISO 306 | |
| Flammability, UL94 | V-2 <br>@Thickness 0.800 mm |
V-2 <br>@Thickness 0.0315 in |
UL 94 |
| V-0 <br>@Thickness 2.00 mm |
V-0 <br>@Thickness 0.0787 in |
UL 94 | |
| 5VB <br>@Thickness 2.30 mm |
5VB <br>@Thickness 0.0906 in |
UL 94 | |
| 5VB <br>@Thickness 2.30 mm |
5VB <br>@Thickness 0.0906 in |
UL 94 by SABIC-IP | |
| Oxygen Index | 29 % | 29 % | ISO 4589 |
| Glow Wire Test | 960 °C <br>@Thickness 1.00 mm |
1760 °F <br>@Thickness 0.0394 in |
IEC 60695-2-12 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Ball Pressure Test, 75°C +/- 2°C | PASSES | IEC 60695-10-2 |