Reliance Industries Repol H020EG Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Reliance Industries
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Reliance Industries Repol H020EG Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
REPOL Polypropylene H020EG is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific catalyst system. Repol H020EG is recommended for use in Extrusion & Blow Molding processes. It is an ideal material for making blow molded bottles, straws, ball pen refills, strappings, stationery items, sheets and thermoformed containers.Features:Good processing stabilityHigh melt strengthInformation provided by Reliance Industries
Physical Properties Metric English Comments
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 34.0 MPa
4930 psi
50mm/min; ASTM D638
Elongation at Yield 10 %
10 %
50mm/min; ASTM D638
Flexural Modulus 1.70 GPa
247 ksi
1% secant; ASTM D790A
Izod Impact, Notched 0.400 J/cm

@Temperature 23.0 °C
0.749 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 104 °C
219 °F
ASTM D648