Hexcel® HexWeb® CFC™-20-1/8-5.0 Composite Flooring Honeycomb Core

Category Other Engineering Material , Composite Core Material , Polymer , Thermoset , Aramid
Manufacturer Hexcel
Trade Name HexWeb®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexWeb® CFC™-20-1/8-5.0 Composite Flooring Honeycomb Core.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Designation: Material-Cell Size-Density.Hexweb CFC™-20 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes and, after expanding to the hexagonal confiation, the block is dipped in phenolic resin. After curing the resin, slices are cut to the desired thickness.Features: Specifically designed for aircraft flooring applications; Superior properties and performance over balsa and foam core materials; Proven durability in extensive flooring tests; Significant weight advantage over balsa and foam core materials; Exceeds all FAA safety requirements; Excellent property retention at 350°F; Moisture and fungus resistant.Applications: Hexweb CFC™-20 honeycomb core was specifically developed to provide a tough, lightweight core material for use in aircraft flooring systems. A range of product densities are available to fit a wide variety of loading requirements. The core material when bonded to metallic or nonmetallic facings provides a flooring panel sheet which may be cut or contoured to fit any aircraft flooring module.
Physical Properties Metric English Comments
Density 0.0801 g/cc
0.00289 lb/in³
Mechanical Properties Metric English Comments
Compressive Yield Strength >= 3.52 MPa
>= 510 psi
Bare, min
>= 3.79 MPa
>= 550 psi
Stabilized, min
4.83 MPa
700 psi
Bare, typ
5.14 MPa
745 psi
Stabilized, typ
Shear Modulus 0.0448 GPa
6.50 ksi
Plate Shear, W Direction, typ, preliminary value obtained from limited testing
0.0827 GPa
12.0 ksi
Plate Shear, L Direction, typ, preliminary value obtained from limited testing
Shear Strength >= 1.10 MPa
>= 160 psi
Plate Shear, W Direction, min, preliminary value obtained from limited testing
1.41 MPa
205 psi
Plate Shear, W Direction, typ, preliminary value obtained from limited testing
>= 1.86 MPa
>= 270 psi
Plate Shear, L Direction, min, preliminary value obtained from limited testing
2.45 MPa
355 psi
Plate Shear, L Direction, typ, preliminary value obtained from limited testing