Material Notes:
PA6 30% Glass Fiber and mineral filler reinforced injection molding grade. Good stiffness and good dimensional stability. Heat stabilized, good surface finish.Information provided by Radici group.
Mechanical Properties Metric English Comments
Tensile Strength at Break 65.0 MPa
9430 psi
Elongation at Break 2.9 %
2.9 %
Tensile Modulus 6.25 GPa
906 ksi
Charpy Impact Unnotched 4.90 J/cm²

@Temperature -30.0 °C
23.3 ft-lb/in²

@Temperature -22.0 °F
5.20 J/cm²

@Temperature 23.0 °C
24.7 ft-lb/in²

@Temperature 73.4 °F
Charpy Impact, Notched 0.550 J/cm²

@Temperature -30.0 °C
2.62 ft-lb/in²

@Temperature -22.0 °F
0.850 J/cm²

@Temperature 23.0 °C
4.04 ft-lb/in²

@Temperature 73.4 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
Comparative Tracking Index 550 V
550 V
Users viewing this material also viewed the following: