| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.26 g/cc | 0.0455 lb/in³ | DIN 53479 |
| Filler Content | 13 - 17 % | 13 - 17 % |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | <= 120 MPa | <= 17400 psi | 50 mm/min; ISO 527-1,2 |
| Elongation at Break | 4.0 % | 4.0 % | ISO 527-1,2 |
| Charpy Impact Unnotched | <= 2.50 J/cm² @Temperature 23.0 °C |
<= 11.9 ft-lb/in² @Temperature 73.4 °F |
DIN 53453 |
| Charpy Impact, Notched | <= 1.00 J/cm² @Temperature -20.0 °C |
<= 4.76 ft-lb/in² @Temperature -4.00 °F |
DIN 53453 |
| <= 1.00 J/cm² @Temperature 23.0 °C |
<= 4.76 ft-lb/in² @Temperature 73.4 °F |
DIN 53453 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 250 °C | 482 °F | DIN 53461 |
| Deflection Temperature at 1.8 MPa (264 psi) | 220 °C | 428 °F | DIN 53461 |
| Flammability, UL94 | HB @Thickness 4.00 mm |
HB @Thickness 0.157 in |
MSZ 10383 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | DIN 53482 |
| Comparative Tracking Index | 375 V | 375 V | IEC 112 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Moisture Content | 1.5 - 1.8 % | 1.5 - 1.8 % | DIN 53714 |