Momentive Performance Materials FSE7340 Heat Cured Fluorosilicone Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Momentive Performance Materials (Former GE Silicones)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Momentive Performance Materials FSE7340 Heat Cured Fluorosilicone Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance standards.Fluorosilicones are suitable for applications in presence of fuel, oils, blow by gas, and various solvents. FSE7340 is a peroxide curable, high tear resistance grade silicone elastomer.All Fluorosilicones are available as customized ready-to-use products.
Physical Properties Metric English Comments
Specific Gravity 1.44 g/cc
1.44 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 43
43
Tensile Strength 11.2 MPa
1620 psi
Elongation at Break 500 %
500 %
Tear Strength 42.0 kN/m
240 pli
Die B
Compression Set 8.0 %
8.0 %
Descriptive Properties Value Comments
Appearance Pale Yellow