| Category | Polymer , Thermoplastic , Nylon , Nylon 612 |
| Manufacturer | Quadrant Engineering Plastics Products |
| Trade Name | Quadrant Nylon |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Quadrant EPP Quadrant Nylon 612.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.10 g/cc | 1.10 g/cc | ASTM D792 |
| Water Absorption | 0.20 % | 0.20 % | IMMERSION, 24 HRS.; ASTM D570 2 |
| Water Absorption at Saturation | 3.0 % | 3.0 % | ASTM D570 2 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength | 72.4 MPa | 10500 psi | ASTM D638 |
| Elongation at Break | 35 % | 35 % | ASTM D638 |
| Tensile Modulus | 2.92 GPa | 424 ksi | ASTM D638 |
| Flexural Strength | 88.3 MPa | 12800 psi | ASTM D638 |
| Flexural Modulus | 2.79 GPa | 405 ksi | ASTM D790 |
| Compressive Strength | 82.7 MPa @Strain 10.0 %, Temperature 22.8 °C |
12000 psi @Strain 10.0 %, Temperature 73.0 °F |
ASTM D695 |
| Compressive Modulus | 1.83 GPa | 265 ksi | ASTM D695 |
| Shear Strength | 55.2 MPa | 8000 psi | ASTM D732 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 216 °C | 420 °F | ASTM D3418 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Constant | 3.2 | 3.2 | ASTM D150 |