| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Strength | 88.3 MPa | 12800 psi | ASTM D790 |
| PolyOne Geon™ Vinyl Packaging 4195 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
| Flexural Strength | 88.5 MPa | 12800 psi | ASTM D790 |
| PolyOne Geon™ Vinyl Rigid Extrusion 87547 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
| Flexural Strength | 88.5 MPa | 12800 psi | ASTM D790 |
| PolyOne Geon™ Vinyl Rigid Extrusion 87554 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
| Flexural Strength | 88.3 MPa | 12800 psi | ASTM D790 |
| Owens Corning Glass Fiber Reinforced Polyester SMC (Compression), 22 wt.% glass Polyester thermosets are available in many formulations. They can be formulated for good to excellent resistance to acids, weak alkalis, and organic solvents. However, they are not recommended for u.. |
|||
| Flexural Strength | 88.0 MPa | 12800 psi | ASTM D790 |
| LG Chemical LUCEL EC-605B Electrically Conductive POM, 5% Carbon Black Filled LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
| Flexural Strength | 88.3 MPa | 12800 psi | ASTM D790 |
| Kolon DIAMAT® EM Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
| Flexural Strength | 88.0 MPa | 12800 psi | ASTM D790 |
| Kotec Carbotex K-75E Polycarbonate, Extrusion Grade Features: Extrusion, High viscosity, Natural transparentApplications: Sheets FilmsInformation provided by Kotec Corporation |
|||
| Flexural Strength | 88.0 MPa | 12800 psi | ASTM D790 |
| LG Chemical LUPOY GP-1000 General Purpose Modified PC, Unreinforced Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
| Flexural Strength | 88.0 MPa | 12800 psi | ASTM D790 |
| Gromax CCP PBT 1100-104S Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
| Flexural Strength | 88.0 MPa | 12800 psi | ISO 178 |
| SABIC Innovative Plastics LNP STAT-KON DX11408 PC LNP* STAT-KON* DX11408 is a compound based on Polycarbonate containing Carbon Powder. Added features of this material include: Electrically Conductive, Improved Ductility |
|||
| Flexural Strength | 88.3 MPa | 12800 psi | ASTM D790 |
| Techmer ES Luriblend® TPX-POM-01060 Availability: North AmericaForms: PelletsAdditive: LubricantFeatures: Lubricated and Good Wear ResistanceAppearance: BlackInformation provided by TP Composites, Inc. |
|||
| Flexural Strength | 88.3 MPa | 12800 psi | 2.8 mm/min; ASTM D790 |
| Samsung Cheil Industries Infino® EF-1032 PC/ABS, Unreinforced FR Extrusion resin, non-halogen flame-retardantInformation provided by Samsung Cheil Industries. |
|||
| Flexural Strength | 88.3 MPa | 12800 psi | 2.8 mm/min; ASTM D790 |
| Samsung Cheil Industries Infino® NH-1023P PC, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
| Flexural Strength | 88.3 MPa | 12800 psi | 2.8 mm/min; ASTM D790 |
| Samsung Cheil Industries Infino® NH-1035 PC, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
| Flexural Strength | 88.3 MPa | 12800 psi | 2.8 mm/min; ASTM D790 |
| Samsung Cheil Industries Infino® TP-1002 PC, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
| Flexural Strength | 88.3 MPa | 12800 psi | 2.8 mm/min; ASTM D790 |
| Samsung Cheil Industries Infino® NF-3017 PC/ABS, Unreinforced FR Flame-retardant scratch resistant material that can be used in notebook B partInformation provided by Samsung Cheil Industries. |
|||
| Flexural Strength | 88.3 MPa | 12800 psi | 2.8 mm/min; ASTM D790 |
| Samsung Cheil Industries Infino® NH-1027HF PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
| Flexural Strength | 88.3 MPa | 12800 psi | 2.8 mm/min; ASTM D790 |
| Samsung Cheil Industries Infino® NH-1035 PC, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
| Flexural Strength | 88.0 MPa | 12800 psi | ASTM Test |
| Styrolution Terluran® HH-112 ABS Terluran HH-112 is an injection molding grade of ABS with very high heat resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
| Flexural Strength | 88.0 MPa | 12800 psi | ISO 178 |
| SABIC Innovative Plastics LNP Lubricomp XL004 Amorphous Polyamide LNP* Lubricomp* XL-4040 is a compound based on Amorphous Nylon, containing PTFE.This data was supplied by SABIC-IP for the Americas region. |
|||
| Flexural Strength | 88.3 MPa | 12800 psi | ASTM D790 |
| Saint-Gobain Meldin® 7001 Direct Formed Polyimide Finished parts and basic shapes made from unfilled polyimide material for structural applications requiring requiring high electrical insulative properties, high purity and low outgassing, and high .. |
|||
| Flexural Strength | 88.3 MPa | 12800 psi | 2.8 mm/min; ASTM D790 |
| Samsung Cheil Industries Infino® SI-3109GL PC, Glass Filled High Impact Information provided by Samsung Cheil Industries. |
|||
| Flexural Strength | 88.0 MPa | 12800 psi | ASTM D790 |
| Plenco 2308 Phenolic, Granular, Transfer Molded PLENCO 02308 is a general purpose organic filled phenolic molding compound, offering improved heat resistance and optimized cure properties. UL recognized under component file E40654. 02308 is avai.. |
|||
| Flexural Strength | 88.3 MPa | 12800 psi | Yeild; ASTM D790 |
| CPC - Vycom VINTEC I® PVC Polyvinyl Chloride (PVC) Vintec I is a normal impact, high corrosion resistant polyvinyl chloride (PVC) sheet. Because of its exceptional corrosion resistance, it is ideally suited for applications where maximum chemical re.. |
|||
| Flexural Strength | 88.0 MPa | 12800 psi | 23°C, 50% RH; ASTM D790 |
| Asahi Kasei Xyron® 600H Modified Polyphenylene Ether Heat ResistantInformation provided by Asahi Kasei |
|||
| Flexural Strength | 88.3 MPa | 12800 psi | Yeild; ASTM D790 |
| CPC - Vycom Ultra White™ PVC Advanced, UV (Ultra Violet) resistant sheet Ultra White is an advanced PVC formulation designed specifically for outdoor applications where resistance to ultraviolet (UV) degradation is critical. Tests show that Ultra White retards both surfa.. |
|||
| Flexural Strength | 88.0 MPa | 12800 psi | ISO 178 |
| Polyplastics Duracon® M270-45 Acetal Co-polymer (POM), Weather resistance, High flow, High cycle DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
| Flexural Strength | 88.0 MPa | 12800 psi | ISO 178 |
| Lucite International Diakon® Frost 902 80 Acrylic Polymer Information provided by Lucite International |
|||