| Category | Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, MoS2 Filled |
| Manufacturer | Quadrant Engineering Plastics Products |
| Trade Name | Nylatron® |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Quadrant EPP Nylatron® GSM Nylon, Cast MoS2 Filled Type 6 (ASTM Product Data Sheet).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.16 g/cc | 1.16 g/cc | ASTM D792 |
| Water Absorption | 0.60 % | 0.60 % | Immersion, 24hr; ASTM D570(2) |
| Water Absorption at Saturation | 7.0 % | 7.0 % | Immersion; ASTM D570(2) |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell M | 80 | 80 | ASTM D785 |
| Hardness, Rockwell R | 110 | 110 | ASTM D785 |
| Hardness, Shore D | 85 | 85 | ASTM D2240 |
| Tensile Strength | 75.8 MPa | 11000 psi | ASTM D638 |
| Elongation at Break | 30 % | 30 % | ASTM D638 |
| Tensile Modulus | 2.76 GPa | 400 ksi | ASTM D638 |
| Flexural Strength | 110 MPa | 16000 psi | ASTM D790 |
| Flexural Modulus | 3.45 GPa | 500 ksi | ASTM D790 |
| Compressive Strength | 96.5 MPa | 14000 psi | 10% Def.; ASTM D695 |
| Compressive Modulus | 2.76 GPa | 400 ksi | ASTM D695 |
| Shear Strength | 72.4 MPa | 10500 psi | ASTM D732 |
| Izod Impact, Notched | 0.267 J/cm | 0.500 ft-lb/in | ASTM D256 Type A |
| Coefficient of Friction, Dynamic | 0.20 | 0.20 | Dry vs. Steel; QTM55007 |
| K (wear) Factor | 181 x 10<sup>-8</sup> mm³/N-M | 90.0 x 10<sup>-10</sup> in³-min/ft-lb-hr | QTM 55010 |
| Limiting Pressure Velocity | 0.105 MPa-m/sec | 3000 psi-ft/min | 4:1 safety factor; QTM 55007 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 90.0 µm/m-°C @Temperature -40.0 - 149 °C |
50.0 µin/in-°F @Temperature -40.0 - 300 °F |
ASTM E831 |
| Melting Point | 216 °C | 420 °F | Crystalline, Peak; ASTM D3418 |
| Maximum Service Temperature, Air | 93.3 °C | 200 °F | Long Term |
| Deflection Temperature at 1.8 MPa (264 psi) | 93.3 °C | 200 °F | ASTM D648 |
| Flammability, UL94 | HB | HB | 1/8 inch (Estimated Rating) |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Surface Resistivity per Square | >= 1.00e+13 ohm | >= 1.00e+13 ohm | EOS/ESD S11.11 |
| Dielectric Constant | 3.7 @Frequency 1e+6 Hz |
3.7 @Frequency 1e+6 Hz |
ASTM D150 |
| Dielectric Strength | 15.7 kV/mm | 400 kV/in | Short Term; ASTM D149 |
| Compliance Properties | Metric | English | Comments |
|---|---|---|---|
| 3A-Dairy | No | No | |
| Canada AG | No | No | |
| FDA | No | No | |
| NSF | No | No | |
| USDA | No | No | |
| USP Class VI | No | No |
| Chemical Resistance Properties | Metric | English | Comments |
|---|---|---|---|
| Acids, Strong (pH 1-3) | Unacceptable | Unacceptable | |
| Acids, Weak | Limited | Limited | |
| Alcohols | Limited | Limited | |
| Alkalies, Strong (pH 11-14) | Unacceptable | Unacceptable | |
| Alkalies, Weak | Limited | Limited | |
| Chlorinated Solvents | Limited | Limited | |
| Conductive / Static Dissipative | No | No | |
| Continuous Sunlight | Limited | Limited | |
| Hot Water / Steam | Limited | Limited | |
| Hydrocarbons - Aliphatic | Acceptable | Acceptable | |
| Hydrocarbons - Aromatic | Acceptable | Acceptable | |
| Inorganic Salt Solutions | Acceptable | Acceptable | |
| Ketones, Esters | Acceptable | Acceptable |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Color | Black-Grey | |
| Machinability | 1 | 1-10, 1=Easier to Machine |