Henkel Frekote B-15 Sealer Mold Sealer

Category Fluid , Polymer
Manufacturer Henkel
Trade Name Frekote
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Henkel Frekote B-15 Sealer Mold Sealer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Formulated as a sealer for molds with microporosity problems, small surface scratches or imperfections. Used in conjunction with other Frekote products, Frekote B-15 provides an excellent base coat, enhancing the release advantages of all Frekote products.Benefits: Seals mold porosity No contaminating transfer Compatible with all Frekote products
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 60.0 °C
140 °F
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 125 °C
1.00 hour

@Temperature 257 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F