| Category | Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, Carbon Fiber Filled |
| Manufacturer | Quadrant Engineering Plastics Products |
| Trade Name | Ketron® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Quadrant EPP Ketron® CA30 LSG PEEK, Extruded 30% Carbon Fiber Reinforced Polyetherether Ketone (ASTM Product Data Sheet).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.41 g/cc | 1.41 g/cc | ASTM D792 |
| Water Absorption | 0.060 % | 0.060 % | Immersion, 24hr; ISO 62 |
| Water Absorption at Saturation | 0.30 % | 0.30 % |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell M | 102 | 102 | ISO 2039-2 |
| Hardness, Shore D | 93 | 93 | |
| Tensile Strength | 131 MPa | 19000 psi | ASTM D638 |
| Elongation at Break | 5.0 % | 5.0 % | ISO 527 |
| Tensile Modulus | 7.58 GPa | 1100 ksi | ASTM D638 |
| Flexural Strength | 177.5 MPa | 25750 psi | ASTM D790 |
| Flexural Modulus | 8.62 GPa | 1250 ksi | ASTM D790 |
| Compressive Strength | 200 MPa | 29000 psi | 10% Def.; ASTM D695 |
| Izod Impact, Notched | 0.550 J/cm | 1.03 ft-lb/in | |
| Charpy Impact Unnotched | 5.00 J/cm² | 23.8 ft-lb/in² | ISO 179-1/1eU |
| Charpy Impact, Notched | 0.500 J/cm² | 2.38 ft-lb/in² | ISO 179-1/1eA |
| Coefficient of Friction, Dynamic | 0.20 | 0.20 | Dry vs. Steel; QTM55007 |
| K (wear) Factor | 302 x 10<sup>-8</sup> mm³/N-M | 150 x 10<sup>-10</sup> in³-min/ft-lb-hr | |
| Limiting Pressure Velocity | 0.876 MPa-m/sec | 25000 psi-ft/min | 4:1 safety factor; QTM 55007 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 18.0 µm/m-°C <br>@Temperature -40.0 - 149 °C |
10.0 µin/in-°F <br>@Temperature -40.0 - 300 °F |
ASTM E831 |
| Thermal Conductivity | 0.922 W/m-K | 6.40 BTU-in/hr-ft²-°F | |
| Melting Point | 340 °C | 644 °F | ISO 11357 |
| Maximum Service Temperature, Air | 250 °C | 482 °F | |
| Deflection Temperature at 1.8 MPa (264 psi) | 270 °C | 518 °F | ISO 75 |
| Minimum Service Temperature, Air | -20.0 °C | -4.00 °F | |
| Flammability, UL94 | V-0 <br>@Thickness 1.50 mm |
V-0 <br>@Thickness 0.0591 in |
|
| V-0 <br>@Thickness 3.00 mm |
V-0 <br>@Thickness 0.118 in |
||
| Oxygen Index | 40 % | 40 % | ISO 4589 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Surface Resistivity per Square | <= 1e+05 | <= 1e+05 | IEC 60093 |
| Dielectric Strength | 1.26 kV/mm | 32.0 kV/in |
| Compliance Properties | Metric | English | Comments |
|---|---|---|---|
| 3A-Dairy | No | No | |
| Canada AG | No | No | |
| FDA | No | No | |
| NSF | No | No | |
| USDA | No | No | |
| USP Class VI | Yes | Yes |
| Chemical Resistance Properties | Metric | English | Comments |
|---|---|---|---|
| Acids, Strong (pH 1-3) | Limited | Limited | |
| Acids, Weak | Acceptable | Acceptable | |
| Alcohols | Acceptable | Acceptable | |
| Alkalies, Strong (pH 11-14) | Acceptable | Acceptable | |
| Alkalies, Weak | Acceptable | Acceptable | |
| Chlorinated Solvents | Acceptable | Acceptable | |
| Conductive / Static Dissipative | Yes | Yes | |
| Continuous Sunlight | Limited | Limited | |
| Hot Water / Steam | Acceptable | Acceptable | |
| Hydrocarbons - Aliphatic | Acceptable | Acceptable | |
| Hydrocarbons - Aromatic | Acceptable | Acceptable | |
| Inorganic Salt Solutions | Acceptable | Acceptable | |
| Ketones, Esters | Acceptable | Acceptable |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Color | Natural |