Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -20.0 °C | -4.00 °F | Recommended |
Nye Lubricants 131A (DMO) Delicate Machinery Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -20.0 °C | -4.00 °F | Recommended |
Nye Lubricants 310B-RP (SO) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -20.0 °C | -4.00 °F | Recommended |
Nye Lubricants 760K (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -20.0 °C | -4.00 °F | Recommended |
Nye Lubricants 794 (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -20.0 °C | -4.00 °F | |
Precision Polymer Engineering V70D Fluoroelastomer Compound Fluoroelastomer Rubber, 66-75 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. Meets Aerospace Specifications DTD5612A and DTD5543B Grade 70.Applications: Mouldings which are requ.. |
|||
Minimum Service Temperature, Air | -20.0 °C | -4.00 °F | |
Precision Polymer Engineering V75M Fluoroelastomer Compound Brown Fluoroelastomer Rubber, 70-80 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. To meet ASTM D2000 line call-out:- M2HK710, A1-10, B37, B38, EF31, EO78, F15, Z1, Z2. Z1 = comp.. |
|||
Minimum Service Temperature, Air | -20.0 °C | -4.00 °F | |
Precision Polymer Engineering V75N Fluoroelastomer Compound Fluoroelastomer Rubber, 71-80 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. Meets Aerospace Specification DTD5543A Grade E. Note: inactive for new design, replaced by DTD5543B .. |
|||
Minimum Service Temperature, Air | -20.0 °C | -4.00 °F | |
Precision Polymer Engineering V90D Fluoroelastomer Compound Fluoroelastomer Rubber, 86-93 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. Meets Aerospace Specifications DTD5612A and DTD5543B Grade 90. ASTM designation = FKM. ISO designatio.. |
|||
Minimum Service Temperature, Air | -20.0 °C | -4.00 °F | |
Precision Polymer Engineering Z75R Hydrogenated NBR Compound Red Hydrogenated Nitrile Rubber, 70-80 °IRHD. Medium acrylonitrile (ACN) content. ASTM designation = HNBR. ASTM D2000 line call-out 2MDH708, A26, B36, EO16, EO36, F14, Z1. Z1 = hardness 75 ±5.Ap.. |
|||
Minimum Service Temperature, Air | -20.0 °C | -4.00 °F | |
Polynorbornene Rubber (PNR) High glass temperature - plasticizer needed to make a 'rubbery' compound. |
|||
Minimum Service Temperature, Air | -20.0 °C | -4.00 °F | |
Manifattura Cattaneo PET Polyethylene Terephthalate Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Minimum Service Temperature, Air | -20.0 °C | -4.00 °F | |
Freudenberg Simrit V189 Non-Black Compound Specific compounding ingredients can reduce or eliminate the presence of carbon black. These compounds may provide improved resistance to oxidative environments and reactive plasmas. The inorganic p.. |
|||
Minimum Service Temperature, Air | -20.0 °C | -4.00 °F | |
Greene Tweed CHEMRAZ® SD625 Perfluoroelastomer Chemraz® SD625, a black-colored perfluoroelastomer, offers the broadest chemical resistance of any elastomer, combining the resilience and sealing force of an elastomer with chemical resistance a.. |
|||
Minimum Service Temperature, Air | -20.0 °C | -4.00 °F | |
Freudenberg Simrit Viton® SC1106 CV75 HP-1 (TFE/P) The lowest elemental extractable fluoroelastomer available. Is based on an acid-resistant fluoroelastomer. Typical used as a coater/ developer, dry etch, wet etch, cleaning, resists stripping, ion i.. |
|||
Minimum Service Temperature, Air | -20.0 °C | -4.00 °F | |
Freudenberg Simrit Viton® SC1107 CV75WH ETP Excellent resistance to most chemicals. The performance of these products is greater than traditional fluoroelastomers. Avoid use in strong bases or amines. Typical used in wet etch, dry etch, CVD, .. |
|||
Minimum Service Temperature, Air | -20.0 °C | -4.00 °F | |
Fujipoly Industries WSL Connector Fujipoly W connector is capable of connecting fine pitch linear pads and pad grid arrays. It is conductive only in the thickness direction which makes it appropriate for low profile "z-axis" connect.. |
|||
Minimum Service Temperature, Air | -20.0 °C | -4.00 °F | |
Trelleborg Emerson & Cuming Eccobond® B 97 Heat Cure Catalyst Emerson & Cuming B 97 Eccobond® Heat Cure CatalystVery high temperature resistance, not as brittle as 17 M 1. Cures from 80°C to 200°C. Excellent chemical resistance. May also be used as an accel.. |
|||
Minimum Service Temperature, Air | -20.0 °C | -4.00 °F | |
Trelleborg Emerson & Cuming Stycast® W-66/17M-1 Two-Component Epoxy High Service Temp Encapsulant Features and Typical ApplicationsAbility to withstand high temperatures, thermal shock, and chemical exposure. These products are designed for heat generating electronic devices which operate in har.. |
|||
Minimum Service Temperature, Air | -20.0 °C | -4.00 °F | JIS-K-6723 |
Denka VINYKON W4029 PVC, W grade for equipment cords, for heat resistance A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |
|||
Minimum Service Temperature, Air | -20.0 °C | -4.00 °F | DSC |
Adamas Adalon® 205 PTFE, 15/5% Glass/MoS2 Filled Information provided by Adamas, HPM |
|||
Minimum Service Temperature, Air | -20.0 °C | -4.00 °F | |
ATG s.r.l. ACM Polyacrylic Rubber |
|||
Minimum Service Temperature, Air | -20.0 °C | -4.00 °F | |
CENTROPLAST CENTROMID 6.6 GF 30 Polyamide 6.6 30% glass fiber This material has very high strength and rigidity, with lower moisture absorption. It can be used for housing parts, threaded bolts, and distance pieces.Information provided by CENTROPLAST Engineer.. |
|||
Minimum Service Temperature, Air | -20.0 °C | -4.00 °F | |
Murtfeldt Murylat® SP Polyethylene Terephthalate Murylat® SP combines the properties of Murylat® with improved wear and friction characteristics. It also has increased dynamic resilience which, for example, significantly reduces the required dri.. |
|||
Minimum Service Temperature, Air | -20.0 °C | -4.00 °F | |
Trelleborg Commercial Neoprene® C803 Chloroprene CR or Chloroprene is a homopolymer of chloroprene or chlorobutadiene. NEOPRENE®PropertiesExcellent mechanical and abrasion properties even without reinforcing fillers.Reasonable resilience in grade.. |
|||
Minimum Service Temperature, Air | -20.0 °C | -4.00 °F | ASTM D 3575 |
Eurofoam Porocell POR 302/T-E NBR/PVC Foam Acrylonitrile butadiene and polyvinyl chloride foam rubber. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurof.. |
|||
Minimum Service Temperature, Air | -20.0 °C | -4.00 °F | |
Precision Polymer Engineering V60V Fluoroelastomer Compound Special steam resistant, Black Fluoroelastomer Rubber, 55-65 °IRHD. Terpolymer of vinylidene fluoride, hexafluoropropylene and tetrafluoroethylene. To meet ASTM D2000 line call-out: MHK610, A1-10.. |