Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear = 130 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 130 µm/m-°C

@Temperature 20.0 °C
72.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Network Polymers Kepital® F30-03
Description: Natural Acetal CopolymerInformation provided by Network Polymers Inc.
CTE, linear 130 µm/m-°C

@Temperature 20.0 °C
72.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Network Polymers Kepital® F40-03
Description: Natural Acetal CopolymerInformation provided by Network Polymers Inc.
CTE, linear 130 µm/m-°C

@Temperature 20.0 °C
72.2 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Petromont 1000 High Density Polyethylene Resin
Petromont HDPE 1000 is a high density polyethylene copolymer resin produced using the Unipol® Process. This multi-purpose resin can be used on intermittent and continuous blow moulding machines to ..
CTE, linear 130 µm/m-°C

@Temperature 20.0 °C
72.2 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Petromont 5000 High Density Polyethylene Resin
Petromont HDPE 5000 is a high density polyethylene copolymer resin produced using the UNIPOL™ Process. This resin is intended for use in prime sheet and thermoforming applications such as arena boa..
CTE, linear 130 µm/m-°C
72.2 µin/in-°F
Above Tg
EVALCA EVAL® LC-E151B Ethylene Vinyl Alcohol Copolymer Resin  (discontinued **)
44 mol % Ethylene.Data provided by EVALCA. Applications: Melt phase forming, solid phase pressure forming, blow molding, tubes EVOH is used in packaging applications because of its outstanding gas..
CTE, linear 130 µm/m-°C
72.2 µin/in-°F
ASTM D696
Kolon KOCETAL® DS500 Acid Resistant Acetal Resin
Improved acid resistance. Applications: Products for improved chemical resistance. Information provided by API-Kolon.
CTE, linear 130 µm/m-°C
72.2 µin/in-°F
ASTM D696
Kolon KOCETAL® EL304 Toughened Grade Acetal Resin
Flexible grade. Applications: Flexible products. Information provided by API-Kolon.
CTE, linear 130 µm/m-°C
72.2 µin/in-°F
ASTM D696
Kolon KOCETAL® K300EW Standard Grade Acetal Resin
General injection molding grade, toughness is slightly improved. Applications: General injection molding products.Information provided by API-Kolon.
CTE, linear 130 µm/m-°C
72.2 µin/in-°F
ASTM D696
Kolon KOCETAL® K500 Standard Grade Acetal Resin
General injection molding grade. Easy flow grade for hard-to fill molds and mechanical thin-wall parts.Applications: General injection molding products.Information provided by API-Kolon.
CTE, linear 130 µm/m-°C
72.2 µin/in-°F
ASTM D696
Kolon KOCETAL® LF701 Wear Modified Acetal Resin
Special polymer added, improved wear property. Applications: Products for low noise and precision gear. Information provided by API-Kolon.
CTE, linear 130 µm/m-°C
72.2 µin/in-°F
ASTM D696
Kolon KOCETAL® VT702 Anti-Static Grade Acetal Resin
Improved antistatic effects. Applications: Products for avoiding electric contamination. Information provided by API-Kolon.
CTE, linear 130 µm/m-°C

@Temperature 23.0 - 55.0 °C
72.2 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-2
Polyplastics Duracon® AW-01 Acetal Co-polymer (POM), High sliding, Special lubricant, High sliding
DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O)..
CTE, linear 130 µm/m-°C

@Temperature 20.0 °C
72.2 µin/in-°F

@Temperature 68.0 °F
TMA
Toyobo PELPRENE™ S2002FB Polyester TPE, Flame Resistant
Features: Polyester TPE, Flame ResistantInformation provided by Toyobo.
CTE, linear 130 µm/m-°C
72.2 µin/in-°F
Above Tg
Tra-Con Tra-Bond 342-14T Low Viscosity Room Temperature Cure Epoxy Adhesive
TRA-BOND 342-14T single component, low viscosity alumina-filled epoxy adhesive exhibits high bond strength and excellent thermal shock characteristics. This adhesive may be cured at room temperature..
CTE, linear 130 µm/m-°C

@Temperature -30.0 - 100 °C
72.2 µin/in-°F

@Temperature -22.0 - 212 °F
3M Scotch-Weld™ 2214 Non-Metallic Filled Epoxy Adhesive
3M™ Scotch-Weld™ Non-Metallic Filled is a non-metal filled version of Scotch-Weld adhesive 2214 regular. One part 250°F (121°C) curing 100% solids, 3M™ Scotch-Weld™ Epoxy Adhesive 2214 is a pa..
CTE, linear 130 µm/m-°C

@Temperature 20.0 °C
72.2 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Asahi Glass Fluon® P-805UP PFA Perfluoropolymer
Fluon® PFA is a copolymer of tetrafluoroethylene (C2F4) and perfluoroalkoxyethylene, which has excellent chemical, electrical, mechanical and surface properties. PFA retains many inherent character..
CTE, linear 130 µm/m-°C
72.2 µin/in-°F
Hippe PVDF
Better mechanical strength compared to other fluorinated polymers. Tough and hard. High-grade electrical feature. Good weathering stability. Physiologically safe. Not as good as fluorinated pol..
CTE, linear 130 µm/m-°C

@Temperature 23.0 - 55.0 °C
72.2 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-2
Polyplastics Duracon® SF-10 Acetal Co-polymer (POM), High impact, Flexible
DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O)..
CTE, linear 130 µm/m-°C

@Temperature 23.0 - 55.0 °C
72.2 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-2
Polyplastics Duracon® HP25X Acetal Co-polymer (POM), High stiffness, High viscosity