| Category | Polymer , Thermoplastic , Nylon , Nylon 6 |
| Manufacturer | Polykemi AB |
| Trade Name | SCANMID 6 |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Polykemi AB SCANMID 6 B12^ F Nylon 6.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.13 g/cc | 0.0408 lb/in³ | ISO 1183 |
| Linear Mold Shrinkage | 0.012 cm/cm | 0.012 in/in | With Flow; ISO 2577 |
| 0.014 cm/cm | 0.014 in/in | Across Flow; ISO 2577 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 77 <br>@Time 15.0 sec |
77 <br>@Time 0.00417 hour |
ASTM D2240 |
| Tensile Strength at Break | <= 75.0 MPa | <= 10900 psi | ISO/R527 |
| Elongation at Break | 40 % | 40 % | ISO/R527 |
| Elongation at Yield | 4.0 % | 4.0 % | ISO/R527 |
| Flexural Strength | <= 105 MPa | <= 15200 psi | ISO 178 |
| Flexural Modulus | 2.60 GPa <br>@Temperature 23.0 °C |
377 ksi <br>@Temperature 73.4 °F |
ISO 178 |
| Charpy Impact, Notched | 0.600 J/cm² <br>@Temperature 23.0 °C |
2.86 ft-lb/in² <br>@Temperature 73.4 °F |
ISO 179 |
| 0.600 J/cm² <br>@Temperature -20.0 °C |
2.86 ft-lb/in² <br>@Temperature -4.00 °F |
ISO 179 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 180 °C | 356 °F | 120°C/h; ISO 75/1 |
| Deflection Temperature at 1.8 MPa (264 psi) | 65.0 °C | 149 °F | 120°C/h; ISO 75/1 |
| Vicat Softening Point | 200 °C <br>@Load 5.001 kg |
392 °F <br>@Load 11.03 lb |
50°C/h; ISO 306 |
| Flammability, UL94 | V-2 <br>@Thickness 1.60 mm |
V-2 <br>@Thickness 0.0630 in |
|
| Glow Wire Test | 750 °C <br>@Thickness 2.00 mm |
1380 °F <br>@Thickness 0.0787 in |
IEC 695-2-1 |