| Category | Polymer , Thermoplastic , Nylon , Nylon 66 |
| Manufacturer | Polykemi AB |
| Trade Name | SCANAMID 66 |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Polykemi AB SCANAMID 66 A12^F Nylon 66.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.14 g/cc | 0.0412 lb/in³ | ISO 1183 |
| Linear Mold Shrinkage | 0.011 cm/cm | 0.011 in/in | With Flow; ISO 2577 |
| 0.015 cm/cm | 0.015 in/in | Across Flow; ISO 2577 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 79 @Time 15.0 sec |
79 @Time 0.00417 hour |
ASTM D2240 |
| Tensile Strength at Break | <= 90.0 MPa | <= 13100 psi | ISO/R527 |
| Elongation at Break | 25 % | 25 % | ISO/R527 |
| Elongation at Yield | 5.5 % | 5.5 % | ISO/R527 |
| Flexural Strength | <= 140 MPa | <= 20300 psi | ISO 178 |
| Flexural Modulus | 3.10 GPa @Temperature 23.0 °C |
450 ksi @Temperature 73.4 °F |
ISO 178 |
| Charpy Impact, Notched | 0.500 J/cm² @Temperature -20.0 °C |
2.38 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
| 0.600 J/cm² @Temperature 23.0 °C |
2.86 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 210 °C | 410 °F | 120°C/h; ISO 75/1 |
| Deflection Temperature at 1.8 MPa (264 psi) | 75.0 °C | 167 °F | 120°C/h; ISO 75/1 |
| Vicat Softening Point | >= 210 °C @Load 5.001 kg |
>= 410 °F @Load 11.03 lb |
50°C/h; ISO 306 |
| Flammability, UL94 | V-2 @Thickness 1.60 mm |
V-2 @Thickness 0.0630 in |
|
| Glow Wire Test | 750 °C @Thickness 2.00 mm |
1380 °F @Thickness 0.0787 in |
IEC 695-2-1 |