| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Vicat Softening Point | 135 °C @Load 1.00 kg |
275 °F @Load 2.21 lb |
50°C/h; ISO 306 |
| Polykemi AB POLYfill PP EIP2012 F Polypropylene, Mineral Reinforced, Extrusion grade, Low CLTE Information provided by Polykemi AB |
|||
| Vicat Softening Point | 135 °C @Load 1.00 kg |
275 °F @Load 2.21 lb |
50°C/h; ISO 306 |
| Polykemi AB POLYfill PPC K20010 PP, 10% Mineral Reinforced Information provided by Polykemi AB |
|||
| Vicat Softening Point | 135 °C @Load 1.00 kg |
275 °F @Load 2.21 lb |
50°C/h; ISO 306 |
| Polykemi AB POLYfill PPC K5025 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
| Vicat Softening Point | 135 °C @Load 1.00 kg |
275 °F @Load 2.21 lb |
50°C/h; ISO 306 |
| Polykemi AB POLYfill PPC K5025 PP, Mineral Reinforced Information provided by Polykemi AB |
|||
| Vicat Softening Point | 135 °C @Load 1.00 kg |
275 °F @Load 2.21 lb |
50°C/h; ISO 306 |
| Polykemi AB POLYfill PPHC K2040H Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
| Vicat Softening Point | 135 °C @Load 1.00 kg |
275 °F @Load 2.21 lb |
50°C/h; ISO 306 |
| Polykemi AB POLYlux 3709M PC/PBT-Blend Information provided by Polykemi AB |
|||
| Vicat Softening Point | 135 °C @Load 1.00 kg |
275 °F @Load 2.21 lb |
50°C/h; ISO 306 |
| Polykemi AB POLYlux 3709MLB PC/PBT-Blend, Paintable Information provided by Polykemi AB |
|||
| Vicat Softening Point | 135 °C @Load 1.00 kg |
275 °F @Load 2.21 lb |
50°C/h; ISO 306 |
| Polykemi AB SCANBLEND FS7 FR UV PC/ASA Blend, Flame-Retardant, UV Stabilized Information provided by Polykemi AB |
|||
| Vicat Softening Point | 135 °C @Load 1.00 kg |
275 °F @Load 2.21 lb |
50°C/h; ISO 306 |
| Polykemi AB SCANBLEND SS7 PC/ASA, UV-Resistant Information provided by Polykemi AB |
|||
| Vicat Softening Point | 135 °C @Load 1.00 kg |
275 °F @Load 2.21 lb |
50°C/h; ISO 306 |
| Polykemi AB POLYfill PPC K6020 S Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
| Vicat Softening Point | 135 °C @Load 1.02 kg |
275 °F @Load 2.25 lb |
ISO 306 |
| Borealis EE002AE Polypropylene Elastomer Modified EE002AE is a reactor elastomer modified polypropylene compound intended for injection molding. The product is available in natural color. This material has excellent balanced mechanical properties.. |
|||
| Vicat Softening Point | 135 °C @Load 5.10 kg |
275 °F @Load 11.2 lb |
ISO 306 |
| Borealis GB311U Polypropylene Compound, Glass Fiber Reinforced GB311U is a 30% chemically coupled glass fiber reinforced polypropylene compound intended for injection molding. This material shows excellent mechanical properties also at elevated temperatures. .. |
|||
| Vicat Softening Point | 135 °C @Load 5.10 kg |
275 °F @Load 11.2 lb |
ISO 306 |
| Borealis GB364WG Polypropylene Compound, Glass Fiber Reinforced GB364WG is a 30% chemically coupled glass fiber reinforced polypropylene compound intended for injection molding. The product is available in natural but other colors can be provided on request. Th.. |
|||
| Vicat Softening Point | 135 °C @Load 5.10 kg |
275 °F @Load 11.2 lb |
ISO 306 |
| Borealis GB366WG Polypropylene Compound, Glass Fiber Reinforced GB366WG is a 30% chemically coupled glass fiber reinforced polypropylene compound intended for injection molding. The product is available in natural but other colors can be provided on request. Th.. |
|||
| Vicat Softening Point | 135 °C @Load 5.10 kg |
275 °F @Load 11.2 lb |
ISO 306 |
| Borealis GD310U Polypropylene Compound, Glass Fiber Reinforced GD310U is a 30% chemically coupled glass fiber reinforced polypropylene compound intended for injection molding. This material shows excellent mechanical properties also at elevated temperatures. .. |
|||
| Vicat Softening Point | 135 °C @Load 1.02 kg |
275 °F @Load 2.25 lb |
50°C per hour; ISO 306 |
| Total PPC 7810 Polypropylene, Heterophasic Copolymer, High Impact Polypropylene PPC 7810 is a very high impact heterophasic copolymer with a Melt Flow index of 15 g/10 min.Polypropylene PPC 7810 has been specially developed for high impact and heavy duty applicati.. |
|||
| Vicat Softening Point | 135 °C @Load 1.02 kg |
275 °F @Load 2.25 lb |
50°C per hour; ISO 306 |
| Total PPC 8780 Polypropylene, Heterophasic Copolymer, Injection Molding Polypropylene PPC 8780 is a controlled rheology heterophasic copolymer with a Melt Flow index of 18 g/10 min.Polypropylene PPC 8780 has been specially developed for the injection molding of lids com.. |
|||
| Vicat Softening Point | 135 °C @Load 1.02 kg |
275 °F @Load 2.25 lb |
50°C per hour; ISO 306 |
| Total PPC 3060 MW5 Polypropylene, Heterophasic Copolymer, Automotive Polypropylene AUTOMOTIVE PPC 3060 MW5 is a heterophasic copolymer with a Melt Flow index of 7 g/10 min.Polypropylene AUTOMOTIVE PPC 3060 MW5 is a high impact copolymer with heat stabilization packag.. |
|||
| Vicat Softening Point | 135 °C @Load 0.999 kg |
275 °F @Load 2.20 lb |
50°C/hr; ASTM D 1525 |
| Cossa Polimeri ESTABLEND 4500 T V0 Flame Retardant PC - ABS PC - ABS BlendFlame retardant class V0, PBDE free, with halogens, high impact resistance, high thermal resistance, good processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
| Vicat Softening Point | 135 °C @Load 0.999 kg |
275 °F @Load 2.20 lb |
50°C/hr; ASTM D 1525 |
| Cossa Polimeri ESTABLEND 6500 A Polycarbonate ABS Blend Polycarbonate and Acrylonitrile Butadiene Styrene blendHigh thermal resistance, high impact resistanceInformation provided by Cossa Polimeri S.r.l. |
|||
| Vicat Softening Point | 135 °C @Load 0.999 kg |
275 °F @Load 2.20 lb |
50°C/hr; ASTM D 1525 |
| Cossa Polimeri ESTABLEND 6500 F Polycarbonate ABS Blend Polycarbonate and Acrylonitrile Butadiene Styrene blendHigh melt flow rate, good thermal resistance, good impact resistance, excellent processability, good surface appearanceInformation provided by .. |
|||
| Vicat Softening Point | 135 °C @Load 0.999 kg |
275 °F @Load 2.20 lb |
50°C/hr; ASTM D 1525 |
| Cossa Polimeri ESTABLEND 6500 Polycarbonate ABS Blend Polycarbonate and Acrylonitrile Butadiene Styrene blendHigh thermal resistance, high impact resistanceInformation provided by Cossa Polimeri S.r.l. |
|||
| Vicat Softening Point | 135 °C @Load 0.999 kg |
275 °F @Load 2.20 lb |
50°C/hr; ASTM D 1525 |
| Cossa Polimeri ESTABLEND 8500 V0 HF Flame Retardant PC - ABS PC - ABS BlendFlame retardant class V0, chlorine and bromine free, good light resistance, good thermal and mechanical properties, excellent processabilityInformation provided by Cossa Polimeri S.r.l.. |
|||
| Vicat Softening Point | 135 °C @Load 0.999 kg |
275 °F @Load 2.20 lb |
120°C/hr; ASTM D 1525 |
| Cossa Polimeri ESTABLEND PSA 6600 PC / ASA Blend Polycarbonate and acrylonitrile styrene acrylate blendGood light resistance, good impact resistance, high heat resistance, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
| Vicat Softening Point | 135 °C @Load 5.00 kg |
275 °F @Load 11.0 lb |
120°C/hr; ASTM D 1525 |
| Cossa Polimeri ESTABLEND PSA 8500 V0 Flame Retardant PC / ASA Blend Polycarbonate and acrylonitrile styrene acrylate blendFlame retardant class V0, excellent light resistance, high impact resistance, excellent processabilityInformation provided by Cossa Polimeri S.r.. |
|||