| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Screw Speed | 80 - 120 rpm | 80 - 120 rpm | |
|
PolyOne Versaflex™ HC 2110-57B Thermoplastic Elastomer (TPE)
Versaflex™ HC 2110-57B is a TPE designed for use in the healthcare industry offering low stiction and good compression set. New Product. Commercial specifications have not been established. - Bonds..
|
|||
| Screw Speed | 80 - 120 rpm | 80 - 120 rpm | |
|
PolyOne Versaflex™ HC MT555 Thermoplastic Elastomer (TPE)
Versaflex™ HC MT555 is an easy processing material designed for applications where FDA compliance and medical testing is required. - Excellent Colorability - Soft TouchRear: 340 - 360F Center: 380 ..
|
|||
| Screw Speed | 80 - 120 rpm | 80 - 120 rpm | |
|
PolyOne Versaflex™ OM 6059-9 Thermoplastic Elastomer (TPE)
Versaflex™ OM 6059-9 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Except..
|
|||
| Screw Speed | 80 - 120 rpm | 80 - 120 rpm | |
|
PolyOne Versaflex™ OM 6240-1 Thermoplastic Elastomer (TPE)
Versaflex™ OM 6240-1 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Except..
|
|||
| Screw Speed | 80 - 120 rpm | 80 - 120 rpm | |
|
PolyOne Versaflex™ OM 6258-1 Thermoplastic Elastomer (TPE)
Versaflex™ OM 6258-1 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Except..
|
|||
| Screw Speed | 80 - 120 rpm | 80 - 120 rpm | |
|
PolyOne Versaflex™ OM 6258-9 Thermoplastic Elastomer (TPE)
Versaflex™ OM 6258-9 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Except..
|
|||
| Screw Speed | 80 - 120 rpm | 80 - 120 rpm | |
|
PolyOne Versaflex™ OM 6275-1 Thermoplastic Elastomer (TPE)
Versaflex™ OM 6275-1 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. New Prod..
|
|||
| Screw Speed | 80 - 120 rpm | 80 - 120 rpm | |
|
PolyOne Versaflex™ VDT 4132 Thermoplastic Elastomer (TPE)
Versaflex™ VDT 4132 is designed to create vibration damping. - Excellent Vibration DampingRear = 350-370F Middle = 375-400F Front = 375-400F Nozzle = 365-380F Screw speed = 100-500rpmPurge thorough..
|
|||
| Screw Speed | 80 - 125 rpm | 80 - 125 rpm | |
|
NOVA Chemicals Dylark® 238P20 High Performance Glass Filled Styrenic
Very high modulus, High heat resistance, Excellent flow characteristics, Excellent adhesion to urethaneApplications: Instrument panel substrates, consoles, Cluster housing, interior trimInjection Sp..
|
|||
| Screw Speed | 80 - 125 rpm | 80 - 125 rpm | |
|
NOVA Chemicals Dylark® 378P15 Glass Reinforced Engineering Resin
Features: Very high modulus, High heat resistance, excellent flow characteristics, excellent adhesion to urethaneApplications: Instrument panel substrates, Consoles, Cluster housings, Interior trim
|
|||
| Screw Speed | 80 - 125 rpm | 80 - 125 rpm | |
|
NOVA Chemicals Dylark® 378P30 Glass Reinforced Engineering Resin
Features: Ultra high modulus, High heat resistance, excellent adhesion to urethaneApplications: Instrument panel substrates, Brackets, Structural components
|
|||
| Screw Speed | 80 - 125 rpm | 80 - 125 rpm | |
|
NOVA Chemicals Dylark® 480P12 High Performance Glass Filled Styrenic
Very high modulus, High heat resistance, Excellent flow characteristics, Excellent adhesion to urethaneApplications: Instrument panel substrates, consoles, Cluster housing, interior trimInjection Sp..
|
|||
| Screw Speed | 80 - 125 rpm | 80 - 125 rpm | |
|
NOVA Chemicals DYLARK® 480P16 Glass Reinforced Engineering Resin
Features:Very high modulus High heat resistance Excellent flow characteristics Excellent adhesion to urethaneApplications:Instrument panel substrates Consoles Cluster housings Interior trimInformati..
|
|||
| Screw Speed | 80 - 160 rpm | 80 - 160 rpm | |
|
PolyOne Bergamid™ XP6042701 Polyamide 6 (Nylon 6)
Injection Speed: 50 to 80% Holding Time: 3 to 9 sec Injection Time: 1 to 3.5 sec Cycle Time: 18 to 60 secInformation provided by PolyOne
|
|||
| Screw Speed | 80 - 120 rpm | 80 - 120 rpm | |
|
PolyOne Edgetek® XP9242701 Polyphenylene Sulfide (PPS)
Injection Speed: 50 to 80% Holding Time: 3 to 9 sec Injection Time: 1 to 3 sec Cycle Time: 18 to 70 secInformation provided by PolyOne
|
|||
| Screw Speed | 80 - 125 rpm | 80 - 125 rpm | |
|
NOVA Chemicals Dylark® 250P20 High Performance Glass Filled Styrenic
Very high modulus, High heat resistance, Excellent flow characteristics, Excellent adhesion to urethaneApplications: Instrument panel substrates, consoles, Cluster housing, interior trimInjection Sp..
|
|||
| Screw Speed | 80 - 125 rpm | 80 - 125 rpm | |
|
NOVA Chemicals Dylark® 378P20 High Performance Glass Filled Styrenic
Very high modulus, High heat resistance, Excellent flow characteristics, Excellent adhesion to urethaneApplications: Instrument panel substrates, consoles, Cluster housing, interior trimInjection Sp..
|
|||
| Screw Speed | 80 - 125 rpm | 80 - 125 rpm | |
|
NOVA Chemicals Dylark® 480P20 High Performance Glass Filled Styrenic
Very high modulus, High heat resistance, Excellent flow characteristics, Excellent adhesion to urethaneApplications: Instrument panel substrates, consoles, Cluster housing, interior trimInjection Sp..
|
|||
| Screw Speed | 80 - 125 rpm | 80 - 125 rpm | |
|
NOVA Chemicals Dylark® 510XT Glass Reinforced Engineering Resin
Features: Higher toughness product, Excellent stiffness, High heat resistance, Superior adhesion to urethane foamApplications: Instrument panel substrates, Mid-Consoles, Center Stacks, Interior tri..
|
|||
| Screw Speed | 80 - 125 rpm | 80 - 125 rpm | |
|
NOVA Chemicals Dylark® 520XT Glass Reinforced Engineering Resin
Features: Higher toughness product, Excellent stiffness, High heat resistance, Superior adhesion to urethane foamApplications: Instrument panel substrates, Mid-Consoles, Center Stacks, Interior tri..
|
|||
| Screw Speed | <= 80 rpm | <= 80 rpm | Injection Molding |
|
LG Chemical LG703W ABS, Low Gloss, Heat Resistance
Feature: Injection Molding, Low Gloss, Heat ResistanceApplication: Automobiles Interior Housing (Column Cover, Filllar Etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided..
|
|||
| Screw Speed | <= 80 rpm | <= 80 rpm | Injection Molding |
|
LG Chemical LG704W ABS, Low Gloss, Heat Resistance
Feature: Injection Molding, Low Gloss, Heat ResistanceApplication: Automobiles Interior Housing (Column Cover, Filllar Etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Information provided by LG Chem..
|
|||
| Screw Speed | <= 80 rpm | <= 80 rpm | Injection Molding |
|
LG Chemical LG709W ABS, Low Gloss, Heat Resistance
Injection Molding, Low Gloss, Heat ResistanceApplication: Automobiles Interior Housing (Column Cover, Pilllars, Etc.)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG..
|
|||
| Screw Speed | <= 80 rpm | <= 80 rpm | Injection Molding |
|
LG Chemical LG749W ABS, Low Gloss, Heat Resistance
Feature: Injection Molding, Low Gloss, Heat ResistanceApplication: Automotive Interior Housing (Glove Cover, Door S/W Housing Etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Information provided by..
|
|||
| Screw Speed | <= 80 rpm | <= 80 rpm | Injection Molding |
|
LG Chemical LI942 Heat Resistant ASA
Description: High Heat ASAApplication: Automotive Part (Roof Rack Cover)CAS: 26299-47-8Information provided by LG Chemical
|
|||
| Screw Speed | <= 80 rpm | <= 80 rpm | Injection Molding |
|
LG Chemical LI951 Heat Resistant ASA
Description: High Heat ASAApplication: Automotive Part (Radiator Grill, Side Mirror)CAS: 26299-47-8Information provided by LG Chemical
|
|||
| Screw Speed | 80 - 110 rpm | 80 - 110 rpm | Injection Molding |
|
LG Chemical LUCEL HI525L POM+Rubber, High Impact
Feature: Injection Molding, POM+Rubber, High ImpactApplication: GearsCAS No. 66455-31-0 and 155123-66-3Information provided by LG Chemical
|
|||
| Screw Speed | <= 80 rpm | <= 80 rpm | Injection Molding |
|
LG Chemical LUCON TR1000 PMMA+CNT
Description: Injection Molding, PMMA+CNT, Transparency, Permanent Antistatic, Low OutgassingApplication: Wafer Carrier Cover, Pellicle TrayCAS No. 9010-94-0 and 25053-09-2Information provided by LG ..
|
|||
| Screw Speed | <= 80 rpm | <= 80 rpm | Injection Molding |
|
LG Chemical MP220 ABS, High Adhesion, Heat Resistance
Feature: Injection Molding, High Adhesion, Metal PlatingApplication: Automobiles Radiator Grill, MoldingCAS No. 9003-56-9 and 9003-54-7Information provided by LG Chemical
|
|||
| Screw Speed | 80 - 100 rpm | 80 - 100 rpm | |
|
Clariant Renol PCSP0019 Polycarbonate/Acrylic Alloy
Data provided by Clariant Masterbatches
|
|||