| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1000 ohm-cm - 1e+05 | 1000 ohm-cm - 1e+05 | ASTM D257 |
|
PolyOne Stat-Tech™ AS-13CF/000 Black Acrylonitrile Butadiene Styrene (ABS)
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound..
|
|||
| Volume Resistivity | <= 1000 ohm-cm | <= 1000 ohm-cm | ISO D-257 |
|
Premix Thermoplastics PRE-ELEC® PE 1297 Conductive Thermoplastic Compound
PRE-ELEC® PE 1297 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC® PE..
|
|||
| Volume Resistivity |
<=
1000
ohm-cm <br>@Thickness 0.400 mm
|
<=
1000
ohm-cm <br>@Thickness 0.0157 in
|
ISO D-257 |
|
Premix Thermoplastics PRE-ELEC® PP 1397 Conductive Thermoplastic Compound
PRE-ELEC® PP 1397 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-E..
|
|||
| Volume Resistivity | 1000 - 1.00e+8 ohm-cm | 1000 - 1.00e+8 ohm-cm | ASTM D257 |
|
Solvay Specialty Polymers Hyflon® PFA C920-0020X Perfluoroalkoxy (PFA)
Hyflon® PFA C920-0020X is a semi crystalline, melt processable perfluoroalkoxy fluorocarbon resin specifically designed for applications where the unique properties of PFAs must be combined with ..
|
|||
| Volume Resistivity | 1000 - 1.00e+6 ohm-cm | 1000 - 1.00e+6 ohm-cm | ASTM D257 |
|
SABIC Innovative Plastics LNP STAT-KON DX11408 PC
LNP* STAT-KON* DX11408 is a compound based on Polycarbonate containing Carbon Powder. Added features of this material include: Electrically Conductive, Improved Ductility
|
|||
| Volume Resistivity | 1000 - 10000 ohm-cm | 1000 - 10000 ohm-cm | SABIC Method |
|
SABIC Innovative Plastics NORYL GTX GTX8720 PPE+PA (Asia Pacific)
Noryl GTX* GTX8720 resin is a glass filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-..
|
|||
| Volume Resistivity | 1000 - 10000 ohm-cm | 1000 - 10000 ohm-cm | SABIC Method |
|
SABIC Innovative Plastics NORYL GTX GTX975 PPE+PA (Europe-Africa-Middle East)
NORYL GTX975 is a 18% mineral filled material especially designed for in- or on-line painted exterior automotive trim part, e.g. tankflaps and corner panels. This material combines high stiffness an..
|
|||
| Volume Resistivity | 1000 ohm-cm | 1000 ohm-cm | 8% Carbon Black in HDPE |
|
TIMCAL ENSACO™ 350G Conductive Carbon Black
ENSACO™ & SUPER P™ conductive carbon blacks are carbon blacks with a high to very high void volume allowing the retention of a carbon network at low to very low filler content. The void volume can..
|
|||
| Volume Resistivity | 1000 ohm-cm | 1000 ohm-cm | ASTM D4325 |
|
3M Scotch® 13 Electrical Semi-Conducting Tape
Scotch® Electrical Semi-Conducting Tape 13 is a highly conformable, semi-conducting EPR (Ethylene Propylene Rubber) based high-voltage splicing tape. It is non-vulcanizing and shelf stable, with st..
|
|||
| Volume Resistivity | 1000 ohm-cm - 1e+05 | 1000 ohm-cm - 1e+05 | ASTM D257 |
|
PolyOne Stat-Tech™ PI-05CF/000 EM Polyetherimide (PEI)
(discontinued **)
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound..
|
|||
| Volume Resistivity | 1000 ohm-cm - 1e+05 | 1000 ohm-cm - 1e+05 | ASTM D257 |
|
SABIC Innovative Plastics LNP STAT-KON QEL329 PA 6/10
LNP STAT-KON* QEL329 is a compound based on Nylon 6/10 resin containing 10% Carbon Fiber, 15% PTFE. Added features of this material include: Electrically Conductive, Wear Resistant, Flame Retardant..
|
|||
| Volume Resistivity | 1000 ohm-cm - 1e+05 | 1000 ohm-cm - 1e+05 | ASTM D257 |
|
SABIC Innovative Plastics LNP STAT-KON QEL329 PA 6/10 (Asia Pacific)
LNP STAT-KON* QEL329 is a compound based on Nylon 6/10 resin containing Carbon Fiber, Flame Retardant, PTFE. Added features of this material include: Electrically Conductive.
|
|||