Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Volume Resistivity = 1000 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity <= 1000 ohm-cm
<= 1000 ohm-cm
ISO D-257
Premix Thermoplastics PRE-ELEC® PBT 1455
PRE-ELEC PBT 1455 is a conductive thermoplastic compound based on PBT. Conductivity is achieved by using special conductive carbon black. PRE-ELEC PBT 1455 has excellent mechanical properties as wel..
Volume Resistivity <= 1000 ohm-cm
<= 1000 ohm-cm
ISO D-257
Premix Thermoplastics PRE-ELEC® PE 1200 Conductive Thermoplastic Compound
PRE-ELEC® PE 1200 is a conductive thermoplastic masterbatch/compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. PRE-ELEC® PE 1200 has a high concentration o..
Volume Resistivity <= 1000 ohm-cm
<= 1000 ohm-cm
ISO D-257
Premix Thermoplastics PRE-ELEC® PE 1299 Conductive Thermoplastic Compound
PRE-ELEC® PE 1299 is a conductive thermoplastic masterbatch/compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. PRE-ELEC® PE 1299 has a high concentration o..
Volume Resistivity <= 1000 ohm-cm

@Thickness 0.400 mm
<= 1000 ohm-cm

@Thickness 0.0157 in
ISO D-257
Premix Thermoplastics PRE-ELEC® PP 1397 Conductive Thermoplastic Compound
PRE-ELEC® PP 1397 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-E..
Volume Resistivity <= 1000 ohm-cm
<= 1000 ohm-cm
ISO D-257
Premix Thermoplastics PRE-ELEC® PS 1326
PRE-ELEC PS 1326 is a conductive thermoplastic compound based on polystyrene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC ..
Volume Resistivity <= 1000 ohm-cm
<= 1000 ohm-cm
ISO D-257
Premix Thermoplastics PRE-ELEC® 12-031  (discontinued **)
PRE-ELEC 12-031 is a conductive thermoplastic compound based on a polyacetal copolymer with 10% carbon fiber. PRE-ELEC 12-031 exhibits excellent mechanical properties and electrical conductivity. Te..
Volume Resistivity 1000 ohm-cm
1000 ohm-cm
ASTM D257
LNP ULTEM® UCF1205 Polyetherimide, 12% Carbon Fiber Reinforcement, 5% PTFE Lubricant  (discontinued **)
Office equipment internal parts.Features: Lubricated, Good Wear ResistanceForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labe..
Volume Resistivity 1000 ohm-cm
1000 ohm-cm
LATI Latigray 82-03 CW/95 PA 12, Metallic Reinforced
Radiopaque compound based on Polyamide 12 (PA12). Metallic filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopl..
Volume Resistivity 1000 - 10000 ohm-cm
1000 - 10000 ohm-cm
SABIC Method
SABIC Innovative Plastics NORYL GTX GTX975 PPE+PA (Asia Pacific)
NORYL GTX975 is a 18% mineral filled material especially designed for in- or on-line painted exterior automotive trim part, e.g. tankflaps and corner panels. This material combines high stiffness an..
Volume Resistivity 1000 - 10000 ohm-cm
1000 - 10000 ohm-cm
SABIC Method
SABIC Innovative Plastics NORYL GTX GTX989 PPE+PA
NORYL GTX989 is a conductive and high heat material, especially designed for in- and on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity..
Volume Resistivity 1000 ohm-cm
1000 ohm-cm
15% Carbon Black
TIMCAL ENSACO™ 260G Conductive Carbon Black
ENSACO™ & SUPER P™ conductive carbon blacks are carbon blacks with a high to very high void volume allowing the retention of a carbon network at low to very low filler content. The void volume can..
Volume Resistivity 1000 ohm-cm
1000 ohm-cm
8% Carbon Black in HDPE
TIMCAL ENSACO™ 350G Conductive Carbon Black
ENSACO™ & SUPER P™ conductive carbon blacks are carbon blacks with a high to very high void volume allowing the retention of a carbon network at low to very low filler content. The void volume can..
Volume Resistivity <= 1000 ohm-cm
<= 1000 ohm-cm
Kazanorgsintez P2ES-12 Electrically Conductive Polyethylene Composite
Production Method: P2ES-12 is produced from low density polyethylene, modified by carbon black, rubber and calcium stearate. Application: Designed for production of pipes used for explosive mate..
Copyright © lookpolymers.com All Rights Reserved