Material Notes:
The Nymax® Series of nylon 6/6 compounds have been specifically developed to deliver outstanding performance in a wide range of application areas. These materials are available with a broad range of fillers, glass reinforcement levels, and impact modifiers depending upon grade selected and have been formulated to offer ease of processing in most standard thermoplastic processing equipment.Molded Test Bars: Dry as MoldedInformation provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.09 g/cc
1.09 g/cc
ASTM D792
Density 1.08 g/cc
0.0390 lb/in³
ISO 1183
Water Absorption 1.0 %
1.0 %
24h/23C; ISO 62
1.0 %

@Thickness 3.18 mm
1.0 %

@Thickness 0.125 in
@ 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.020 - 0.023 cm/cm
0.020 - 0.023 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 42.7 MPa
6190 psi
Type I, 5.1 mm/min; ASTM D638
Tensile Strength, Yield 45.5 MPa
6600 psi
ASTM D638
Elongation at Break 40 %
40 %
Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 1.80 GPa
261 ksi
ISO 527-2
1.86 GPa
270 ksi
ASTM D638
Flexural Strength 75.8 MPa
11000 psi
ASTM D790
Flexural Modulus 1.87 GPa
271 ksi
ASTM D790
Izod Impact, Notched 9.10 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
17.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
ASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
Annealed; ISO 75-2/A
60.0 °C

@Thickness 3.18 mm
140 °F

@Thickness 0.125 in
Unannealed; ASTM D648
Descriptive Properties Value Comments
Additive Heat Stabilizer
Impact Modifier
UV Stabilizer
Appearance Grey
Features General Purpose
Impact Modified
Forms Pellets
Generic Material Nylon 66
Generic Name Polyamide 66 (Nylon 66)
Processing Method Injection Molding
Regional Availability North America
South America
Uses Automotive Applications
Construction Applications
Consumer Applications
General Purpose
Industrial Applications
Users viewing this material also viewed the following: