BorsodChem ONGROVIL S-5167 Suspension PVC-Resin

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Uncompounded
Manufacturer BorsodChem Rt.
Trade Name ONGROVIL
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BorsodChem ONGROVIL S-5167 Suspension PVC-Resin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
S-5167 is a suspension type PVC homopolymer of medium molecular mass. It is characterized by a porous particle structure, a narrow range of particle size and a relatively high apparent density. It retains its excellent pourability even after compounding. Field of application: Ongrovil S-5167 is primarily suitable for rigid applications. Its high apparent density makes it especially suitable for the extrusion of rigid tubes and profiles.Information provided by BorsodChem Rt.
Physical Properties Metric English Comments
Apparent Bulk Density 0.570 - 0.610 g/cc
0.0206 - 0.0220 lb/in³
ISO 60:1977
Particle Size 63 µm
63 µm
5% below
250 µm
250 µm
5% above
Collected Volatile Condensable Material <= 0.30 %
<= 0.30 %
ISO 1269:1980
Descriptive Properties Value Comments
# of Impurities max. 20 pcs/9dm2
K-Value 67±1
Pouring Time, sec (max) 20.5
Residual Vinyl-Chloride Content Max 1 mg/kg