| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.42 g/cc | 0.0513 lb/in³ | ISO 1183 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 53.0 MPa @Temperature 23.0 °C |
7690 psi @Temperature 73.4 °F |
ISO 527-2 |
| Elongation at Break | 5.0 % @Temperature 23.0 °C |
5.0 % @Temperature 73.4 °F |
ISO 527-2 |
| Tensile Modulus | 3.20 GPa @Temperature 23.0 °C |
464 ksi @Temperature 73.4 °F |
ISO 527-2 |
| Charpy Impact Unnotched | 2.80 J/cm² @Temperature 23.0 °C |
13.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
| Charpy Impact, Notched | 0.300 J/cm² @Temperature 23.0 °C |
1.43 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 240 °C | 464 °F | Unannealed; ISO 75-2/B |
| Deflection Temperature at 1.8 MPa (264 psi) | 152 °C | 306 °F | Unannealed; ISO 75-2/A |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 280 - 300 °C | 536 - 572 °F | |
| Mold Temperature | 50.0 - 90.0 °C | 122 - 194 °F | |
| Drying Temperature | 80.0 °C | 176 °F | |
| Dry Time | 3.00 - 4.00 hour | 3.00 - 4.00 hour |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Additive | PTFE Lubricant | |
| Features | Lubricated | |
| Filler / Reinforcement | Glass Bead, 25% Filler by Weight | |
| Forms | Pellets | |
| Generic Material | Nylon 66 | |
| Generic Name | Polyamide 66 (Nylon 66) | |
| Processing Method | Injection Molding | |
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| North America | ||
| South America | ||
| Uses | Appliance Components | |
| Conveyor Parts | ||
| Printer Parts |