| Category | Polymer , Thermoplastic , Nylon , Nylon 6/66 |
| Manufacturer | PolyOne Corporation |
| Trade Name | Bergamid™ |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | PolyOne Bergamid™ AB700 UF Polyamide 66/6 Copolymer (Nylon 66/6).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.20 g/cc | 0.0434 lb/in³ | ±0.03 g/cm³; DIN 53479 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 50.0 MPa @Temperature 23.0 °C |
7250 psi @Temperature 73.4 °F |
ISO 527-2/5 |
| Elongation at Break | 20 % @Temperature 23.0 °C |
20 % @Temperature 73.4 °F |
ISO 527-2/5 |
| Tensile Modulus | 1.60 GPa @Temperature 23.0 °C |
232 ksi @Temperature 73.4 °F |
ISO 527-2/1 |
| Charpy Impact Unnotched | NB @Temperature 23.0 °C |
NB @Temperature 73.4 °F |
ISO 179/1eU |
| Charpy Impact, Notched | 0.300 J/cm² @Temperature 23.0 °C |
1.43 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 243 °C | 469 °F | ISO 3146 |
| Maximum Service Temperature, Air | 80.0 °C | 176 °F | Continuous (GTP 50% Tensile); IEC 60216 |
| 180 °C | 356 °F | Short Time; IEC 60216 | |
| Deflection Temperature at 0.46 MPa (66 psi) | 190 °C | 374 °F | Unannealed; ISO 75-2/B |
| Deflection Temperature at 1.8 MPa (264 psi) | 80.0 °C | 176 °F | Unannealed; ISO 75-2/A |
| Flammability, UL94 | V-0 @Thickness 0.400 mm |
V-0 @Thickness 0.0157 in |
ALL; Internal Method |
| Glow Wire Test | 960 °C @Thickness 3.00 mm |
1760 °F @Thickness 0.118 in |
0.4 mm wire; Ignition Temperature; IEC 60695-2-13 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | IEC 60093 |
| Surface Resistance | 1.00e+10 ohm | 1.00e+10 ohm | IEC 60093 |
| Dielectric Constant | 7.0 @Frequency 1.00e+6 Hz |
7.0 @Frequency 1.00e+6 Hz |
IEC 60250 |
| Dielectric Strength | 45.0 kV/mm | 1140 kV/in | IEC 60243-1 |
| Dissipation Factor | 0.30 @Frequency 1.00e+6 Hz |
0.30 @Frequency 1.00e+6 Hz |
IEC 60250 |
| Comparative Tracking Index | 600 V | 600 V | Solution A; IEC 60112 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Features | Flame Retardant | |
| Halogen Free | ||
| Low (to None) Phosphorus Content | ||
| Forms | Pellets | |
| Generic Material | Nylon 66/6 | |
| Generic Name | Polyamide 66/6 Copolymer (Nylon 66/6) | |
| Regional Availability | Africa & Middle East | |
| Asia Pacific | ||
| Europe | ||
| RoHS Compliance | RoHS Compliant |