Material Notes:
Non-lead stabilized semi-rigid insulation compound recommended for Style #1061 applications. Maximum service temperature of 105°C.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.32 - 1.36 g/cc
1.32 - 1.36 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore D 57 - 63
57 - 63
delayed; ASTM D-2240
Tensile Strength, Yield 22.1 MPa
3210 psi
ASTM D-638
Elongation at Yield 264.9 %
264.9 %
Air Aging: 168 hours @ 136°C; 30 mil slabs; UL 1581
300 %
300 %
ASTM D-638
100% Modulus 0.0200 GPa
2.90 ksi
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -8.00 °C
17.6 °F
ASTM D-746
Oxygen Index 28 %
28 %
ASTM D-638
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
50% RH; ASTM D-257
Processing Properties Metric English Comments
Melt Temperature 188 °C