Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Santoprene® 9101-80E Thermoplastic Vulcanizate - Co-extrusion

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Vulcanizate Elastomer (TPV)
Manufacturer Exxon Chemical
Trade Name Santoprene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Santoprene® 9101-80E Thermoplastic Vulcanizate - Co-extrusion.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Product Description: A black thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is designed for coextrusion applications, particularly for the static foot of automotive weatherseal systems like glass run channels. This grade of Santoprene TPV is shear-dependent and can be processed on conventional thermoplastics equipment for extrusion or thermoforming. It is polyolefin based and completely recyclable.Key Features:Recommended for coextruded applications not exposed to UV light.Recommended for applications requiring excellent ozone resistance.Designed for extruding long runs with minimal build-up of material on screen packs or narrow die sections.Applications:Automotive-Seals, Gaskets and Weather SealsProcessing Method: Coextrusion and ThermoformingAvailability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South AmericaInformation provided by ExxonMobil Chemical.
Physical Properties Metric English Comments
Specific Gravity 0.970 g/cc
0.970 g/cc
ASTM D792 and ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
2 mm; ISO 868
Tensile Strength at Break 7.00 MPa
1020 psi
Across Flow; ASTM D412 and ISO 37
Tensile Stress 3.40 MPa

@Strain 100 %
493 psi

@Strain 100 %
Across Flow; ASTM D412 and ISO 37
Elongation at Break 670 %
670 %
Across Flow; ASTM D412 and ISO 37
Compression Set 48 %

@Temperature 70.0 °C,
Time 79200 sec
48 %

@Temperature 158 °F,
Time 22.0 hour
ASTM D395B Type 1 and ISO 188 Type A
Processing Properties Metric English Comments
Die Temperature 204 °C
400 °F
Melt Temperature 177 - 204 °C
350 - 400 °F
Drying Temperature 82.2 °C
180 °F
Dry Time 3 hour
3 hour
Back Pressure 5.00 - 20.0 MPa
725 - 2900 psi