Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil PPU0009F Polypropylene Impact Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Impact Modified; Molded/Extruded
Manufacturer Exxon Chemical
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil PPU0009F Polypropylene Impact Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Product Description: An unstabilized impact copolymer resin designed for automotive and compounding applications.Availability: Europe Processing Method: CompoundingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ISO 1183
Melt Flow 14 g/10 min
14 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Tensile Modulus 1.10 GPa
160 ksi
ISO527-2
Charpy Impact, Notched 0.294 J/cm²

@Temperature -20.0 °C
1.40 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eA
0.399 J/cm²

@Temperature 0.000 °C
1.90 ft-lb/in²

@Temperature 32.0 °F
ISO 179/1eA
0.798 J/cm²

@Temperature 22.8 °C
3.80 ft-lb/in²

@Temperature 73.0 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C
122 °F
ISO 75-2/A
Users viewing this material also viewed the following: