Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 29.6 MPa | 4290 psi | ASTM D1708 |
DSM Biomedical CarboSil® 40 90A Biocompatible Silicone Polycarbonate Urethane
(discontinued **) Combines the biocompatibility and biostability of conventional silicone elastomers with the processability and toughness of thermoplastic urethane elastomers. Noncytotoxic and nonhemolytic. Low-En.. |
|||
Tensile Strength, Ultimate | 29.6 MPa | 4290 psi | ASTM D638 |
Eastman Tenite Acetate 105E2R30025 Natural, Trsp Cellulose Acetate Plasticizer 33%. Weight loss on heating = 3.6% per ASTM D 707. Soluble matter loss = 0.6% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Tensile Strength, Ultimate | 29.6 MPa | 4290 psi | |
3M Scotch-Weld™ 183 B/A Green Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 1838 B/A is a controlled flow product. This epoxy adhesives are two-part, room temperature curing structural adhesives with high shear strengths and excellent envir.. |
|||
Tensile Strength, Ultimate | 29.6 - 54.2 MPa | 4290 - 7850 psi | Average value: 40.2 MPa Grade Count:6 |
Overview of materials for Silicone Polyurethane, Polycarbonate Based This property data is a summary of similar materials in the MatWeb database for the category "Silicone Polyurethane, Polycarbonate Based". Each property range of values reported is minimum and maxim.. |
|||
Tensile Strength, Ultimate | 29.6 MPa | 4290 psi | ASTM D638 |
Buckeye Polymers BP RPP 4012 TU Polypropylene, 40% Mineral Filled UV StabilizedThis Talc-filled product exhibits excellent properties such as high stiffness, surface aesthetics, low coefficient of thermal expansion, low shrinkage, improved scratch and mar resistan.. |