Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 25% Filler by WeightAdditive: Impact Modifier Features: Impact ModifiedProcessing Method: Injection MoldingInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.27 g/cc
0.0459 lb/in³
ASTM D792
Water Absorption 0.90 %

@Time 86400 sec
0.90 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0010 cm/cm

@Thickness 3.17 mm
0.0010 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 112
112
ASTM D785
Tensile Strength, Yield 124 MPa
18000 psi
ASTM D638
Elongation at Break 4.5 %
4.5 %
ASTM D638
Flexural Strength 172 MPa
25000 psi
ASTM D790
Flexural Modulus 6.55 GPa
950 ksi
ASTM D790
Izod Impact, Notched 2.14 J/cm

@Thickness 3.17 mm
4.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 12.6 µm/m-°C
7.00 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 213 °C
415 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 204 °C
400 °F
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 5.00e+15 ohm-cm
5.00e+15 ohm-cm
ASTM D257
Dielectric Strength 15.7 kV/mm
400 kV/in
Method A (Short-Time); ASTM D149