Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 4.00 - 65.0 kJ/m²
1.90 - 30.9 ft-lb/in²
Average value: 45.1 kJ/m² Grade Count:95
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced". Each property range of values repor..
Izod Impact, Notched (ISO) 3.00 - 65.0 kJ/m²

@Temperature -40.0 - 0.000 °C
1.43 - 30.9 ft-lb/in²

@Temperature -40.0 - 32.0 °F
Average value: 27.3 kJ/m² Grade Count:100
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced