Material Notes:
3M™ 700-Series Hybrid Sealant and Hybrid Adhesive Sealant products are one component, moisture curing products which form permanent elastic bonds. They are similar in function as a typical one component polyurethane sealant but are isocyanate-free. 3M Hybrid Sealants and Hybrid Adhesive Sealants bond to a wide variety of materials including plastics, metals, fiberglass, and wood. Differentiated from other high performance sealants as they are very low VOC, have better UV resistance, and have broad substrate adhesion for a wide range of productivity enhancement applications.Information provided by 3M
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
Volatile Organic Compounds (VOC) Content 11 g/l
11 g/l
Mechanical Properties Metric English Comments
Hardness, Shore A 30
30
ASTM C661
Tensile Strength at Break 1.70 MPa
247 psi
ASTM D412
Elongation at Break 300 %
300 %
ASTM D412
100% Modulus >= 0.000600 GPa
>= 0.0870 ksi
ASTM D412
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 90.0 °C
194 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Processing Properties Metric English Comments
Cure Time 25.0 - 30.0 min
0.417 - 0.500 hour
Tack-Free, 50% RH
Shelf Life 6.00 Month
6.00 Month