| Category | Polymer , Thermoplastic , Nylon , Nylon, Flexible Alloy |
| Manufacturer | Network Polymers |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Network Polymers Nylon 0304NL.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.13 g/cc | 1.13 g/cc | ASTM D792 |
| Water Absorption | 1.6 % | 1.6 % | 24 hours Immersion; ASTM D570 |
| Moisture Absorption at Equilibrium | 2.7 % | 2.7 % | 50% RH; ASTM D570 |
| Linear Mold Shrinkage | 0.012 cm/cm | 0.012 in/in | 1/8 in bar; ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 119 | 119 | ASTM D785 |
| Tensile Strength, Yield | 79.3 MPa | 11500 psi | ASTM D638 |
| 21.4 MPa <br>@Temperature 121 °C |
3100 psi <br>@Temperature 250 °F |
ASTM D638 | |
| 125 MPa <br>@Temperature -40.0 °C |
18200 psi <br>@Temperature -40.0 °F |
ASTM D638 | |
| Elongation at Break | 70 % | 70 % | ASTM D638 |
| 8.0 % <br>@Temperature -40.0 °C |
8.0 % <br>@Temperature -40.0 °F |
ASTM D638 | |
| >= 300 % <br>@Temperature 121 °C |
>= 300 % <br>@Temperature 250 °F |
ASTM D638 | |
| Elongation at Yield | 4.0 % | 4.0 % | ASTM D638 |
| Flexural Strength | 108 MPa | 15700 psi | ASTM D790 |
| Flexural Modulus | 2.83 GPa | 410 ksi | ASTM D790 |
| Izod Impact, Notched | 0.534 J/cm | 1.00 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 82.8 µm/m-°C <br>@Temperature 20.0 °C |
46.0 µin/in-°F <br>@Temperature 68.0 °F |
ASTM D696 |
| Melting Point | 216 °C | 420 °F | ASTM D789 |
| Deflection Temperature at 0.46 MPa (66 psi) | 178 °C | 352 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 65.6 °C | 150 °F | ASTM D648 |