| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.33 g/cc | 0.0480 lb/in³ | ISO 1183-A |
| Water Absorption | 0.95 % | 0.95 % | ISO METHOD 62 |
| Linear Mold Shrinkage | 0.015 cm/cm | 0.015 in/in |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 131 MPa | 19000 psi | ISO METHOD 527 |
| Elongation at Break | 8.0 % | 8.0 % | ISO METHOD 527 |
| Flexural Yield Strength | 160 MPa | 23200 psi | ISO METHOD 176 |
| Flexural Modulus | 6.813 GPa | 988.2 ksi | ISO METHOD 178 |
| Izod Impact, Notched | 1.18 J/cm | 2.21 ft-lb/in | ISO METHOD 180 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 221 °C | 430 °F | ISO METHOD 3146C |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Processing Temperature | 250 °C | 482 °F | |
| Rear Barrel Temperature | 225 °C | 437 °F | |
| Middle Barrel Temperature | 230 °C | 446 °F | |
| Front Barrel Temperature | 250 °C | 482 °F | |
| Nozzle Temperature | 250 °C | 482 °F | |
| Mold Temperature | 80.0 °C | 176 °F | |
| Drying Temperature | 76.0 °C | 169 °F |