Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

NOVA Chemicals Novapol® TR-0735-UG Hexene MDPE Rotational Molding Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , MDPE , Medium Density Polyethylene (MDPE), Rotational Molded
Manufacturer NOVA Chemicals
Trade Name Novapol®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NOVA Chemicals Novapol® TR-0735-UG Hexene MDPE Rotational Molding Resin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Features: Good impact properties Excellent processabilityNSF listed for Stds. 14, 24 and 61 Applications: ToysComplex custom partsHome and garden itemsMailboxesInformation provided by Nova Chemicals
Physical Properties Metric English Comments
Density 0.935 g/cc
0.0338 lb/in³
ASTM D792
ESCR 100% Igepal® >= 1000 hour
>= 1000 hour
Condition A; ASTM D1693
ESCR 10% Igepal® 220 hour
220 hour
Condition A; ASTM D1693
Melt Flow 7.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
7.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 17.3 MPa
2510 psi
ASTM D638
Flexural Modulus 0.780 GPa
113 ksi
ASTM D790
Impact Test 67.8 J

@Thickness 3.17 mm
50.0 ft-lb

@Thickness 0.125 in
ARM Method
203 J

@Thickness 6.35 mm
150 ft-lb

@Thickness 0.250 in
ARM Method
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 47.0 °C
117 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 37.3 °C
99.1 °F
ASTM D648
Users viewing this material also viewed the following: