Esstech X-744-0000 2-Hydroxyethyl Methacrylate Phosphate, C6H11O6P

Category Polymer , Adhesive
Manufacturer Esstech
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Esstech X-744-0000 2-Hydroxyethyl Methacrylate Phosphate, C6H11O6P.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
HEMA phosphate is a liquid adhesive system that bonds to and interacts with calcium-containing substrates. Listed on the Toxic Substance Control Act List. CAS # 24599-21-1.Information provided by ESSTECH, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.243 g/cc
1.243 g/cc
Molecular Weight 210.13 g/mol
210.13 g/mol
Optical Properties Metric English Comments
Refractive Index 1.469
1.469
Descriptive Properties Value Comments
Acidity (KOH per g) > 200 mg
MeHQ Inhibitor (ppm) 100