Physical Properties Metric English Comments
Density 0.935 g/cc
0.0338 lb/in³
ASTM D792
Polimeros Mexicanos Rotolene® Diesel Tank Medium Density Polyethylene
Hexene Copolymer Linear Medium Density Polyethylene. This resin is fully UV8 stabilized.High quality Polyethylene compound specially designed for automotive applications, water tanks, diesel tanks a..
Density 0.936 g/cc
0.0338 lb/in³
ASTM D1505
Polimeros Mexicanos Rotolene® ECO-BLACK Linear Medium Density Polyethylene
MDPE Copolymer with UV8 stabilizer, available as black powder.Recommended for rotomolding. Used for manufacture of septic tanks and garbage bins. Recommended for use in combination with ROTOFOAM B..
Density 0.935 g/cc
0.0338 lb/in³
ASTM D792
NOVA Chemicals Novapol® TR-0735-UG Hexene MDPE Rotational Molding Resin
Features: Good impact properties Excellent processabilityNSF listed for Stds. 14, 24 and 61 Applications: ToysComplex custom partsHome and garden itemsMailboxesInformation provided by Nova Chemicals..
Density 0.936 g/cc
0.0338 lb/in³
ASTM D792
NOVA Chemicals Sclair® 14G Butene LMDPE Film Resin
Film Properties. Features: Low gel, good opacity, easy processability.Applications: Overwrap film.Data provided by the manufacturer.
Density 0.935 g/cc
0.0338 lb/in³
ASTM D1505
Reliance Industries Reclair R35042 Polyethylene
Rotational molding Medium Density Polyethylene grade. Characteristics:good toughness, good impact resistance, good environmental stress crack resistance. Applications:chemical tanks, water storage ..
Density 0.935 g/cc
0.0338 lb/in³
ASTM D1505
SABIC R50035 Linear Low Density Polyethylene for Rotational Molding
Product Description: R50035 are Linear Low Density Polyethylene grades designed to provide excellent stress crack resistance, mechanical properties with high rigidity, toughness, gloss and low warp..
Density 0.935 g/cc
0.0338 lb/in³
ASTM D1505
Formosa Plastics Formolene® L63568 Rotational Molding LLDPE  (discontinued **)
Linear Low Density Polyethylene Hexene Copolymer for Rotational Molding Formolene® L63568 is a general-purpose rotational molding linear low density resin made using the BP Gas Phase Process™. The..
Density 0.935 g/cc
0.0338 lb/in³
Exxon Method
ExxonMobil Escorene® LD-705 High EVA Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A fractional melt index, 13.3% vinyl acetate copolymer specialty film resin for applications requiring outstanding heat sealability, strength, and t..
Density 0.936 g/cc
0.0338 lb/in³
ASTM D792
NOVA Chemicals Sclair® 14A Butene MDPE Film Resin  (discontinued **)
Film Properties. Features: Low gel, strength and toughness, broad MW distribution.Applications: Co-extrusion, blending.Data provided by the manufacturer.
Density 0.936 g/cc
0.0338 lb/in³
LyondellBasell Lupolen® 2012 D SW 413 LDPE
Cable sheathingData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Density 0.935 g/cc
0.0338 lb/in³
ASTM D1505
ICO Polymers ICORENEâ„¢ 110-1329 LMDPE Rotational Molding Resin
Description: ICORENE 110-1329 is a linear medium density polyethylene developed for use in rotational molding. This is a very fast processing material that quickly molds out to offer low surface po..
Density 0.935 g/cc
0.0338 lb/in³
ASTM D1505
ICO Polymers ICORENEâ„¢ 115-1323 LMDPE Rotational Molding Resin
Description: ICORENE 115-1323 is a linear medium density polyethylene developed for use in rotational molding. It is an easy processing material with good surface gloss, scratch resistance and gene..
Density 0.935 g/cc
0.0338 lb/in³
ASTM D1505
ICO Polymers ICORENEâ„¢ 115-1649 LMDPE Rotational Molding Resin
Description: ICORENE 115-1649 polyethylene developed for use in rotational molding. It is an easy processing material with good surface gloss, scratch resistance and generally balanced physical pro..
Density 0.935 g/cc
0.0338 lb/in³
ASTM D1505
Micropol Microlin ML53 Linear Polyethylene Rotational Molding Powder
Information provided by Micropol Limited
Density 0.935 g/cc
0.0338 lb/in³
Mixed
ITW Plexus Plexusâ„¢ MA320 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Excellent low temperature and toughness properties.Information provided by Illinois Tool Works.
Density 0.935 g/cc

@Temperature 20.0 °C
0.0338 lb/in³

@Temperature 68.0 °F
LyondellBasell TPNB Tripropylene glycol normal butyl ether
Information provided by Lyondell.
Density 0.935 g/cc
0.0338 lb/in³
ISO 1183
Borealis Borstar® FB1350 Medium Density Polyethylene
Borstar® FB1350 is a linear medium density polyethylene grade combining excellent extrusion properties with high film stiffness. Borstar® FB1350 is well suited for mono- and coextrusion of films ..
Density 0.936 g/cc
0.0338 lb/in³
ExxonMobil method
ExxonMobil Escorene™ UL 00112 Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: UL 00112 is a fractional MI copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: No Applica..
Density 0.936 g/cc
0.0338 lb/in³
ExxonMobil method
ExxonMobil LLDPE LL 8555.24 Linear Low Density Polyethylene Resin
Product Description: LL 8555 is a linear low density hexene copolymer designed to offer superior processability, excellent dimensional control, whiteness and low warpage. This resin is ideally suite..
Density 0.935 g/cc
0.0338 lb/in³
ASTM D792
Dow DOWLEX™ 2036G Linear Low Density Polyethylene
Improved thermal stability for high stiffness film applications Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Information provided by Dow
Density 0.935 g/cc
0.0338 lb/in³
Dow DOWLEX™ 2553 Linear Low Density Polyethylene, Narrow MW Distribution
DOWLEX® 2553 Polyethylene resin is a narrow molecular weight distribution copolymer designed to offer good environmental stress crack resistance and impact strength with excellent stiffness for hou..
Density 0.935 g/cc
0.0338 lb/in³
ExxonMobil method
ExxonMobil Escorene™ LD 706.15 Cast Ethylene Vinyl Acetate Copolymer
Product Description: Escorene Ultra LD 706.15 is a 14.9 wt% vinyl acetate copolymer film resin designed for coextruded cast film applications.Availability: Latin America, North America and South Ame..
Density 0.935 g/cc
0.0338 lb/in³
ExxonMobil method
ExxonMobil Escorene™ LD 708.62 Ethylene Vinyl Acetate Copolymer
Product Description: Escorene Ultra UL 708.62 is a 14.9% VA copolymer film resin. Film made from LD 708.62 exhibits good impact strength and superior heat sealabilty.Availability: Latin America, Nor..
Density 0.935 g/cc
0.0338 lb/in³
ASTM-D1505
Braskem RD34U3 LLDPE Rotomolding Polyethylene
The resin RD34U3 is a linear low-density polyethylene, 1-butene based, with excellent processability and a good balance of stiffness and impact strength. It contains long term UV6 stabilization and ..
Density 0.935 g/cc
0.0338 lb/in³
Arkema Group Evatane® 1040 VN 4 Ethylene Vinyl Acetate
EVA copolymer made by high pressure tubular process. Applications Grade for flexible films with high transparency and high mechanical properties. Examples: thin stretch film for food packaging, coex..
Density 0.935 g/cc
0.0338 lb/in³
AboCure 50-3
Abatron AboCast 7802-1/AboCure 50-3 (40 pbw) Epoxy
AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 50-3 is a clear, slow converter for lower rigidity. It has an HDT of 60°C, variable ratio, ..
Density 0.935 g/cc
0.0338 lb/in³
Arkema Group Evatane® 1005 VN 4 Ethylene Vinyl Acetate
EVA copolymer made by high pressure tubular process. Applications Grade for flexible films with high transparency and very high mechanical properties. Examples: high strength stretch film, greenhous..
Density 0.936 g/cc
0.0338 lb/in³
ASTM D792
NOVA Chemicals Sclair® 94D1 HDPE Extrusion Resin  (discontinued **)
Features: Excellent processability, high stretchability, excellent strength.Applications: Package nettings for produce, Christmas tree wrap and turkey overwrap.Data provided by the manufacturer.
Density 0.936 g/cc
0.0338 lb/in³
ASTM D792
NOVA Chemicals Sclair® 14B1 Butene LMDPE Film Resin  (discontinued **)
Film Properties. Features: Low gel, good clarity, heat resistance and barrier properties.Applications: Lamination, co-extrusion.Data provided by the manufacturer.
Density 0.935 g/cc
0.0338 lb/in³
ASTM D792
Rochling Engineered Plastics Polystone® Reprocessed (UHMW-PE)
Polystone® M is a highly versatile polymer that features: Low coefficient of friction Excellent abrasion resistance High-impact strength Chemical resistance Complies with FDA regulations under the ..