  Online Service   lookpolymers   27660005
Material Notes:
These materials are a novel family of TPV products based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced by dynamic “vulcanization” or cross-linking of silicone polymers within the thermoplastic organic phase and results in a stable droplet type morphology as shown in the TEM micrograph. TPSiV™ combines the elastomeric performance of silicone rubber with the melt re-processability and thermal and chemical resistance of engineering thermoplastics.Thermoplastic polyurethane based TPSiV™ (3010, 3011, 3111, 3040, 3340 grades) combine the benefits of excellent abrasion resistance from the polyurethane as well as the lower coefficient of friction and improved temperature properties from the silicone rubber.TPSiV™ 3111-70A: Designed for good stability in water contact applications and other aqueous solutions. Plasticizer free, and is currently being used in both NSF61 and FDA (Section 177.2600: 'Rubber articles intended for repeated use') applications.Information provided by Multibase, a Dow Corning Company
Physical Properties Metric English Comments
Specific Gravity 1.15 g/cc
1.15 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
10 sec; ASTM D2240
Tensile Strength at Break 15.0 MPa
2180 psi
ASTM D412
Elongation at Break 600 %
600 %
ASTM D412
Tear Strength 45.6 kN/m
260 pli
ASTM D412
Taber Abrasion, mg/1000 Cycles 35
35
ASTM D1044
Compression Set 20 %

@Temperature 22.8 °C,
Time 79200 sec
20 %

@Temperature 73.0 °F,
Time 22.0 hour
Processing Properties Metric English Comments
Rear Barrel Temperature 180 °C
356 °F
Middle Barrel Temperature 190 °C
374 °F
Front Barrel Temperature 200 °C
392 °F
Nozzle Temperature 205 °C
401 °F
Mold Temperature 10.0 - 30.0 °C
50.0 - 86.0 °F
Drying Temperature 80.0 °C
176 °F
Dry Time 2 - 4 hour
2 - 4 hour
Descriptive Properties Value Comments
Injection Rate Fast