Multibase TPSiV™ 3040-70A Thermoplastic Silicone Vulcanizate

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Vulcanizate Elastomer (TPV) , Polyurethane, TP , Silicone, Thermoplastic
Manufacturer Multibase
Trade Name TPSiV™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase TPSiV™ 3040-70A Thermoplastic Silicone Vulcanizate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
These materials are a novel family of TPV products based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced by dynamic “vulcanization” or cross-linking of silicone polymers within the thermoplastic organic phase and results in a stable droplet type morphology as shown in the TEM micrograph. TPSiV™ combines the elastomeric performance of silicone rubber with the melt re-processability and thermal and chemical resistance of engineering thermoplastics.Thermoplastic polyurethane based TPSiV™ (3010, 3011, 3111, 3040, 3340 grades) combine the benefits of excellent abrasion resistance from the polyurethane as well as the lower coefficient of friction and improved temperature properties from the silicone rubber.TPSiV™ 3040-55A / 60A / 65A / 70A / 85A: Plasticizer free, these grades are designed for good flow characteristics and a unique “silky” feel. They are used in injection molding applications, specifically overmolding and co-molding on PC and ABS. They exhibit good abrasion resistance, and good retention of properties in harsh environments. They are commonly used in communication devices, computers, and electronic devices. They “set up” quickly in the mold, thus yielding fairly fast cycle times.Information provided by Multibase, a Dow Corning Company
Physical Properties Metric English Comments
Specific Gravity 1.15 g/cc
1.15 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 68
68
10 sec; ASTM D2240
Tensile Strength at Break 11.7 MPa
1700 psi
ASTM D412
Elongation at Break 600 %
600 %
ASTM D412
Tear Strength 45.6 kN/m
260 pli
ASTM D412
Thermal Properties Metric English Comments
Flammability, UL94 HB
HB
Processing Properties Metric English Comments
Rear Barrel Temperature 180 °C
356 °F
Middle Barrel Temperature 190 °C
374 °F
Front Barrel Temperature 200 °C
392 °F
Nozzle Temperature 205 °C
401 °F
Mold Temperature 10.0 - 30.0 °C
50.0 - 86.0 °F
Drying Temperature 80.0 °C
176 °F
Dry Time 2 - 4 hour
2 - 4 hour
Descriptive Properties Value Comments
Injection Rate Moderate-Fast