| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Thickness | 50.8 microns | 2.00 mil | Silicone |
|
Dielectric Polymers NT-1020 Silicone/Acrylic Double Coated Tape
(discontinued **)
Crosslinked silicone and acrylic adhesive with 2 mil polyester film release liner backing on the silicone side and moisture stable PE coated kraft (60#) on the acrylic side.Features: Chemical resist..
|
|||
| Thickness | 50.8 microns | 2.00 mil | Adhesive |
|
Dielectric Polymers NT-100A89 General Purpose Laminating Adhesive
(discontinued **)
Acrylic adhesive with moisture stable PE coated kraft (89#) liner.Features: Plasticizer migration resistantChemical resistantMoisture resistantApplications: Mounting nameplates, signs, graphic panel..
|
|||
| Thickness | 50.8 microns | 2.00 mil | 2:1 BUR |
|
LyondellBasell Plexar® PX3060 Extrudable Tie-Layer Resin - Anhydride Modified LLDPE
ApplicationsPlexar® tie-layers are chemically modified resins used to bond unlike materials, primarily in packaging and industrial applications. Common adherents include polyethylene resins and ..
|
|||
| Thickness | 50.8 microns | 2.00 mil | |
|
ExxonMobil LD 071.LQ Blown Film Resin
L Product Description: LD 071 Series case wrap film resins combine good processability with excellent strength and good film optics for bundling applications requiring proper shrink performance, tou..
|
|||
| Thickness | 50.8 microns | 2.00 mil | ExxonMobil Method |
|
ExxonMobil Oppalyte™ 50MO747 OPP Film
Product Description: A white opaque biaxially oriented polypropylene film, coated on one side acrylic, one side PVdC. Provides excellent performance on all packaging machines.Availability: Africa & ..
|
|||
| Thickness | 50.8 microns | 2.00 mil | |
|
Dow 608A Low Density Polyethylene (LDPE)
A formulated clarity film resin for thin gauge optical packaging Optimum gauge range: 0.8 - 2.5 mil Complies with U.S. FDA 21 CFR 177.1520 (c) 2.1 Information provided by Dow
|
|||
| Thickness | 50.8 microns | 2.00 mil | |
|
Dow 662I Low Density Polyethylene Resin
Blown Film Resin designed for enhanced bubble stability High melt strength Optimum gauge range: 1.5 - 5.0 mil Complies with U.S. FDA 21 CFR 177.1520 (c) 2.1 Information provided by Dow
|
|||
| Thickness | 50.8 microns | 2.00 mil | |
|
Dow AFFINITY™ PL 1881G Polyolefin Plastomer (POP)
AFFINITY™ PL 1881G Polyolefin Plastomer (POP) is produced via INSITE™ Technologies. It is designed for use in a variety of packaging applications, including high-speed, form-fill-seal products.In..
|
|||
| Thickness | 50.8 microns | 2.00 mil | Side 1; Arlon SQA-TMS-003 |
|
Arlon 680-R3844R 0.084" (2.13 mm) Cured Silicone Coating with Silica-based Substrate
Design/Construction:Side 1: Cured Silicone Coating Substrate: Silica-basedSide 2: Cured Silicone Coating Rubber Application Advantages:Extremely low thermal conductivityThermally stableBondable to s..
|
|||
| Thickness | 50.8 microns | 2.00 mil | without adhesive |
|
3M Controltac™ 3690C Graphic Film with Comply™ Adhesive
This is a 2-mil white, clear or black film for screen printing graphics. The aggressive, pressure activated-adhesive is slideable and repositionable, and has air release channels for fast and easy b..
|
|||
| Thickness | 50.8 microns | 2.00 mil | without adhesive |
|
3M Controltac™ FN180C-10 Graphic Film
2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Flexible; conforms to compound cures, corrugat..
|
|||
| Thickness | 50.8 microns | 2.00 mil | Facestock |
|
3M FM024 Indoor UL Recognized Clear Polyester Overlaminate Label Product
3M™ Indoor UL Recognized Clear Polyester Overlaminate Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester overlami..
|
|||
| Thickness | 50.8 microns | 2.00 mil | Facestock |
|
3M FM063 Indoor UL Recognized Brite Silver Polyester Label Products
3M™ Indoor UL Recognized Brite Silver Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize..
|
|||
| Thickness | 50.8 microns | 2.00 mil | Facestock |
|
3M FM157P Indoor UL Recognized Computer Imprintable Silver Polyester Label Product
3M™ Indoor UL Recognized Computer Imprintable Silver Polyester Label Products are durable high performance materials that offer excellent thermal stability and moisture resistance. These products a..
|
|||
| Thickness | 50.8 microns | 2.00 mil | Liner |
|
3M FM157P Indoor UL Recognized Computer Imprintable Silver Polyester Label Product
3M™ Indoor UL Recognized Computer Imprintable Silver Polyester Label Products are durable high performance materials that offer excellent thermal stability and moisture resistance. These products a..
|
|||
| Thickness | 50.8 microns | 2.00 mil | Facestock |
|
3M FP083 Clear Polypropylene Label Products
3M™ Clear Polypropylene Label Products are biaxially oriented film materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1212, which is a hi..
|
|||
| Thickness | 50.8 microns | 2.00 mil | without adhesive |
|
3M Scotchcal™ 8000-14 Graphic Film
This 2-mil, screen printable film with a pressure sensitive adhesive that can be used on flat and simple curved surfaces. This film withstands severe weather dn handling conditions encountered by co..
|
|||
| Thickness | 50.8 microns | 2.00 mil | without adhesive |
|
3M Scotchcal™ ElectroCut™ 7125-263 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color..
|
|||
| Thickness | 50.8 microns | 2.00 mil | Facestock |
|
3M 7033 Screen Printable Polyester Performance LabelProducts
3M™ Screen Printable Polyester Performance Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These topcoated polyester label st..
|
|||
| Thickness | 50.8 microns | 2.00 mil | Facestock |
|
3M 7238 HP Indigo Optimized Polyester Label Product
3M™ HP Indigo Optimized Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize 3M™ Adhesive..
|
|||
| Thickness | 50.8 microns | 2.00 mil | Total; ASTM D3752 |
|
3M 856 General Purpose Polyester Tape
3M™ General Purpose Polyester Tape 856 is a transparent polyester film tape for edging and reinforcing applications.Information provided by 3M
|
|||
| Thickness | 50.8 microns | 2.00 mil | Backing; ASTM D3752 |
|
3M 8902 Polyester Tape
3M™ Polyester Tape 8902 is made with strong polyester backing and silicone adhesive, allowing it to be used in applications requiring high temperatures or adhesion to silicone treated surfaces. Thi..
|
|||
| Thickness | 50.8 microns | 2.00 mil | without adhesive |
|
3M Controltac™ IJ380Cv3 Wrap Film with Comply™ v3 Adhesive
2-mil white, vinyl film with a luster finish; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Non-visible, air release channels for fast, easy, bubble-free installa..
|
|||
| Thickness | 50.8 microns | 2.00 mil | Facestock |
|
3M FM155 Indoor UL Recognized Computer Imprintable Silver Polyester Label Product
3M™ Indoor UL Recognized Computer Imprintable Silver Polyester Label Products are durable high performance materials that offer excellent thermal stability and moisture resistance. These products a..
|
|||
| Thickness | 50.8 microns | 2.00 mil | without adhesive |
|
3M Scotchcal™ ElectroCut™ 7125-307 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color..
|
|||
| Thickness | 50.8 microns | 2.00 mil | without adhesive |
|
3M Scotchcal™ ElectroCut™ 7125-49 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color..
|
|||
| Thickness | 50.8 microns | 2.00 mil | Tape Only |
|
3M 466XL Extended Liner Tapes
3M™ Extended Liner Tapes have a liner that extends beyond the width of the adhesive to provide easy liner starting and removal. The liners, with the exception of 3M™ Extended Liner Tape 450EK is p..
|
|||
| Thickness | 50.8 microns | 2.00 mil | Facestock |
|
3M FM049 Clear Polyester Label Product
3M™ Clear Polyester Label Products are durable high performance materials that offer excellent thermal stability and moisture resistance. These products are suitable for demanding applications such..
|
|||
| Thickness | 50.8 microns | 2.00 mil | without adhesive |
|
3M Scotchcal™ 1000LF-10 Graphic Film
2-mil vinyl film; Wide color selection; Includes three colors with both a layflat liner and gray adhesive for excellent hiding power and a transparent film with a layflat liner; Pressure-sensitive a..
|
|||
| Thickness | 50.8 microns | 2.00 mil | without adhesive |
|
3M Scotchcal™ ElectroCut™ 7125-88 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color..
|
|||