| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Thickness | 50.8 microns | 2.00 mil | Foil thickness |
|
Parker Chomerics CHO-FOIL CCJ Shielding Tape
Conductive Adhesive Aluminum FoilDescription: Chomerics’ CHO-FOIL® tapes are an economical EMI shielding solution for a variety of commercial uses. The tapes are available in copper, aluminum, or ..
|
|||
| Thickness | 50.8 microns | 2.00 mil | |
|
LyondellBasell Petrothene® NA942000 Low Density Polyethylene, Film Extrusion Grade
PETROTHENE NA942 is a series of resins designed especially for heavy duty film applications, such as bags used to package fertilizer, peat moss, decorative stone and agricultural and construction ma..
|
|||
| Thickness | 50.8 microns | 2.00 mil | Typical; ASTM D374 |
|
DuPont™ Nomex® N196 Paper, 2 mil Nominal Thickness
Nomex® Type N196 is a high floc grade of Nomex® paper. This leads to a high degree of saturability combined with high stiffness and mechanical properties. Type N196 is used where good saturabili..
|
|||
| Thickness | 50.8 microns | 2.00 mil | |
|
DuPont™ Tedlar® TWH20BS3 Satin White Polyvinyl Fluoride Film
Properties of DuPont™ Tedlar® polyvinyl fluoride (PVF) biaxially oriented film include excellent resistance to weathering, outstanding mechanical properties, and inertness towards a wide variety o..
|
|||
| Thickness | 50.8 microns | 2.00 mil | ExxonMobil Method |
|
ExxonMobil Label-Lyte™ 50LL210 OPP Film
Product Description: An uncoated biaxially oriented, transparent polypropylene film for Pressure Sensitive labeling applications.Availability: Africa & Middle East, Asia Pacific and EuropeKey Featur..
|
|||
| Thickness | 50.8 microns | 2.00 mil | Backing |
|
3M 1170 EMI Shielding Tape
3M EMI Shielding Tapes are well suited for applications requiring reliable point-to-point electrical contact, particularly EMI shielding, grounding and static charge draining.Information provided by..
|
|||
| Thickness | 50.8 microns | 2.00 mil | Facestock |
|
3M 7026 Screen Printable Polyester Performance LabelProducts
3M™ Screen Printable Polyester Performance Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These topcoated polyester label st..
|
|||
| Thickness | 50.8 microns | 2.00 mil | Side 2 Layer 1; Arlon SQA-TMS-003 |
|
Arlon 55578XA028 0.0280" Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: LDPESide 2 Layer 2: Uncured Silicone RubberSide 2 Layer 1: Cured Silicone RubberSubstrate: Style 162 FiberglassSide 1: Cured Silicone RubberThis data represents ty..
|
|||
| Thickness | 50.8 microns | 2.00 mil | Side 2, Cured |
|
Arlon 55578XC028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured/Uncured Layers This data Represents typical values for the production material. The data should not be used to write, or in place of, m..
|
|||
| Thickness | 50.8 - 76.2 microns | 2.00 - 3.00 mil | Side 1 |
|
Arlon 70011B016 0.016" (0.406 mm) Uncured Silicone Rubber with Prime Coated Polyester Fabric Substrate
Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place ..
|
|||
| Thickness | 50.8 microns | 2.00 mil | Facestock |
|
3M FP021502 Clear Polypropylene Label Product
3M™ Clear Polypropylene Label Products offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1410, which is a general purpose permanent tackified acrylic t..
|
|||
| Thickness | 50.8 microns | 2.00 mil | Facestock |
|
3M FP083 Clear Polypropylene Label Products
3M™ Clear Polypropylene Label Products are biaxially oriented film materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1212, which is a hi..
|
|||
| Thickness | 50.8 microns | 2.00 mil | Facestock |
|
3M FP0868 Removable Clear Polypropylene Label Products
3M™ Removable Clear Polypropylene Label Products offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive R3500, which is an ultra removable acrylic designed f..
|
|||
| Thickness | 50.8 microns | 2.00 mil | Facestock |
|
3M FP101 Clear Polypropylene Label Product
3M™ Clear Polypropylene Label Products offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1410, which is a general purpose permanent tackified acrylic t..
|
|||
| Thickness | 50.8 microns | 2.00 mil | without adhesive |
|
3M Scotchcal™ 3632-73 Translucent Film
2-mil translucent cast vinyl film; Matte surface finish that eliminates glare and provides uniform color in reflective light; Built in Graphic Protection System (GPS), which is a top coat that incre..
|
|||
| Thickness | 50.8 microns | 2.00 mil | without adhesive |
|
3M Scotchcal™ ElectroCut™ 7125-193 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color..
|
|||
| Thickness | 50.8 microns | 2.00 mil | without adhesive |
|
3M Scotchcal™ ElectroCut™ 7125-197 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color..
|
|||
| Thickness | 50.8 microns | 2.00 mil | without adhesive |
|
3M Scotchcal™ ElectroCut™ 7725-17 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass..
|
|||
| Thickness | 50.8 microns | 2.00 mil | without adhesive |
|
3M Scotchcal™ IJ780Cv3 Graphic Film
2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-sensitive adhesive with non-visible, air release channels for fast, easy, bubble-free installations; Confirms to flat s..
|
|||
| Thickness | >= 50.8 microns | >= 2.00 mil | Side 1 |
|
Arlon 47561R007 0.0075" (0.190 mm) Uncured Rubber
Design/Construction:Side 1: Uncured RubberSide 2: Uncured RubberAppearance: Red silicone gum on fiberglass fabricThis data represents typical values for the production material. The data should not ..
|
|||
| Thickness | 50.8 microns | 2.00 mil | Facestock |
|
3M 7903FL Screen Printable Sheet Polyester Label Material
3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti..
|
|||
| Thickness | 50.8 microns | 2.00 mil | Adhesive |
|
3M 7945MP Hi-Performance Acrylic 200MP
This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia..
|
|||
| Thickness | 50.8 microns | 2.00 mil | Carrier |
|
3M 9496LE High Strength Double Coated Tape with Adhesives 300LSE and 200MP
3M™ Double Coated Tape 9496LE with 3M™ Low Surface Energy Acrylic Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and..
|
|||
| Thickness | 50.8 microns | 2.00 mil | Backside Adhesive |
|
3M 9496LE High Strength Double Coated Tape with Adhesives 300LSE and 200MP
3M™ Double Coated Tape 9496LE with 3M™ Low Surface Energy Acrylic Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and..
|
|||
| Thickness | 50.8 microns | 2.00 mil | Facestock |
|
3M FM041909 White Polyester Label Products
3M™ White Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize 3M™ Adhesive P1480, which ..
|
|||
| Thickness | 50.8 microns | 2.00 mil | Facestock |
|
3M FMV22 Void Polyester Label Products
3M™ Void Polyester Label Products are tamper-indicating stocks designed to provide a “void” message in the facestock when removal is attempted. These void polyester labels utilize 3M™ Adhesive P..
|
|||
| Thickness | 50.8 microns | 2.00 mil | Facestock |
|
3M OFM0802 Outdoor UL Recognized Brite Silver Polyester Label Products
3M™ Outdoor UL Recognized Brite Silver Polyester Label Products are durable high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize..
|
|||
| Thickness | 50.8 microns | 2.00 mil | without adhesive |
|
3M Scotchcal™ ElectroCut™ 7725-85 Graphic Film
2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass..
|
|||
| Thickness | 50.8 microns | 2.00 mil | Backing; ASTM D3752 |
|
3M 8992 Polyester Tape
3M™ Polyester Tape 8992 is a dark green polyester tape with silicone adhesive. It can be used in a large variety of high temperature applications including powdercoat masking, flashbreaker, and bag..
|
|||
| Thickness | 50.8 microns | 2.00 mil | Adhesive |
|
Dielectric Polymers TRANS-SIL® NT-1005 Silicone Transfer Adhesive
(discontinued **)
Crosslinked silicone adhesive with 2 polyester film release liners.Features: Resistant to extreme temperaturesHigh bond strengthChemical resistantApplications: High performance bonding and other app..
|
|||