| Category | Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS) |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | Noryl |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | SABIC Innovative Plastics NORYL SPN410 PPE+PS.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.06 g/cc | 1.06 g/cc | ASTM D792 |
| Water Absorption | 0.070 % @Time 86400 sec |
0.070 % @Time 24.0 hour |
ASTM D570 |
| Linear Mold Shrinkage, Flow | 0.0050 - 0.0070 cm/cm @Thickness 3.20 mm |
0.0050 - 0.0070 in/in @Thickness 0.126 in |
SABIC Method |
| Linear Mold Shrinkage, Transverse | 0.0050 - 0.0070 cm/cm @Thickness 3.20 mm |
0.0050 - 0.0070 in/in @Thickness 0.126 in |
SABIC Method |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 35.0 MPa | 5080 psi | Type I, 50 mm/min; ASTM D638 |
| Elongation at Break | 82 % | 82 % | Type I, 50 mm/min; ASTM D638 |
| Flexural Yield Strength | 55.0 MPa | 7980 psi | 2.6 mm/min, 100 mm span; ASTM D790 |
| Flexural Modulus | 1.83 GPa | 265 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
| Izod Impact, Notched | 3.73 J/cm | 6.99 ft-lb/in | ASTM D256 |
| 1.86 J/cm @Temperature -40.0 °C |
3.48 ft-lb/in @Temperature -40.0 °F |
ASTM D256 | |
| Gardner Impact | 21.0 J | 15.5 ft-lb | ASTM D3029 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 90.0 µm/m-°C @Temperature -40.0 - 95.0 °C |
50.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
| CTE, linear, Transverse to Flow | 90.0 µm/m-°C @Temperature -40.0 - 95.0 °C |
50.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
| Deflection Temperature at 1.8 MPa (264 psi) | 98.0 °C @Thickness 6.40 mm |
208 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
| UL RTI, Electrical | 50.0 °C | 122 °F | UL 746B |
| UL RTI, Mechanical with Impact | 50.0 °C | 122 °F | UL 746B |
| UL RTI, Mechanical without Impact | 50.0 °C | 122 °F | UL 746B |
| Flammability, UL94 | HB @Thickness 1.47 mm |
HB @Thickness 0.0579 in |
UL 94 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Arc Resistance | 60 - 120 sec | 60 - 120 sec | Tungsten; ASTM D495 |
| Comparative Tracking Index | >= 600 V | >= 600 V | UL 746A |
| Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL 746A |
| High Amp Arc Ignition, HAI | 30 - 60 arcs | 30 - 60 arcs | UL 746A |
| High Voltage Arc-Tracking Rate, HVTR | 80.0 - 150 mm/min | 3.15 - 5.91 in/min | UL 746A |