Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer LyondellBasell (former Equistar)
Trade Name Alathon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Alathon® L5876 High Density Polyethylene, Blow Molding Grade.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
ALATHON L5876 is designed for injection blow molding and extrusion blow molding applications where higher gloss than standard grades is required. Regulatory Status: L5876 meets the requirements of the Food and Drug Administration regulation 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "...articles or components of articles intended for use in contact with food. " Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information.Specific recommendations for processing L5876 can only be made when the processing conditions, equipment and end use are known. For further suggestions please contact your Equistar sales representative.This product is from the former Equistar product line.
Physical Properties Metric English Comments
Density >= 0.956 g/cc
>= 0.0345 lb/in³
ASTM D1505
Melt Flow 0.74 g/10 min
0.74 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 66
66
ASTM D2240
Tensile Strength, Yield 28.3 MPa
4100 psi
ASTM D638
Elongation at Break >= 500 %
>= 500 %
ASTM D638
Flexural Modulus 1.34 GPa
195 ksi
ASTM D790
Tensile Impact 85.4 J/cm
160 ft-lb/in
ASTM D1822
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 76.0 °C
169 °F
ASTM D648
Vicat Softening Point 129 °C
264 °F
ASTM D1525
Brittleness Temperature <= -76.0 °C
<= -105 °F
ASTM D746