DuPont Performance Polymers Crastin® CE15315 BK010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled
Manufacturer DuPont Performance Polymers
Trade Name Crastin®
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF DuPont Performance Polymers Crastin® CE15315 BK010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
15% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin CE15315 BK010 is a 15% glass reinforced flame retardant polybutylene terephthalate molding resin. It is recognized as UL94 V-0 at 0.71mm(0.028in).Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.49 g/cc
0.0538 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0070 cm/cm
0.0070 in/in
ISO 294-4 2577
Linear Mold Shrinkage, Transverse 0.010 cm/cm
0.010 in/in
ISO 294-4 2577
Mechanical Properties Metric English Comments
Tensile Strength at Break 91.0 MPa
13200 psi
ISO 527-1/-2
Elongation at Break 2.8 %
2.8 %
ISO 527-1/-2
Tensile Modulus 5.70 GPa
827 ksi
ISO 527-1/-2
Charpy Impact Unnotched 2.31 J/cm²
11.0 ft-lb/in²
ISO 179/1eU
2.15 J/cm²

@Temperature -30.0 °C
10.2 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 0.510 J/cm²
2.43 ft-lb/in²
ISO 179/1eA
0.500 J/cm²

@Temperature -30.0 °C
2.38 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 223 °C
433 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 195 °C
383 °F
ISO 75-1/-2
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
IEC 60695-11-10
V-0

@Thickness 0.700 mm
V-0

@Thickness 0.0276 in
IEC 60695-11-10
Descriptive Properties Value Comments
Part Marking Code >PBT-GF15FR(17)<
ISO 11469
Processing Injection Moulding
Regional Availability Asia Pacific
Resin Identification PBT-GF15FR(17)