Material Notes:
This product is based on Shell's Kraton G and is used for acoustic barrier applications, exhibiting high flexibility and ease of installation. It is made exclusively for Cascade Engineering. This product meets SD2-234 specifications, Harrison Radiator, CMP UP 01 AA, and GM 2217 M. The burn rate is 0.09 in/min (2.25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.89 g/cc
0.0683 lb/in³
ASTM D792
Melt Flow 5.0 g/10 min
5.0 g/10 min
(Condition L) ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore A 89
89
10 sec; ASTM D-2240
Tensile Strength, Ultimate 4.30 MPa
624 psi
ASTM D412
Elongation at Break 350 %
350 %
ASTM D412
Tear Strength 30.0 kN/m
171 pli
ASTM D624