Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 160 °F Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 71.1 °C

@Thickness 3.18 mm
160 °F

@Thickness 0.125 in
Unannealed; ASTM D648
PolyOne Geon™ Vinyl Packaging PK8-1080 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Deflection Temperature at 1.8 MPa (264 psi) 71.0 °C
160 °F
ASTM D648
Nylene® 406 Nylon 6
Injection molding grade. Dry as molded. Nylene 406 is a general purpose, fast cycling molding resin. Crystallization initiators provide fast molding cycles through rapid melt set-up. Parts molded f..
Deflection Temperature at 1.8 MPa (264 psi) 71.0 °C
160 °F
ASTM D648
Nylene® 406F Nylon 6, 50% RH
Injection molding grade. Nylene 406F is a resin formulated to comply with FDA regulation 21 CFR 177.1500 for food contact applications. Nylene 406F is a general purpose, fast cycling molding resin. ..
Deflection Temperature at 1.8 MPa (264 psi) 71.0 °C
160 °F
ASTM D648
Nylene® PA6/6 Impact Modified 311 HS Nylon 6/6
Medium Impact Grade; Property data for dry as molded samples.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Deflection Temperature at 1.8 MPa (264 psi) 71.1 °C
160 °F
ASTM D648
Nilit Polynil® P240HSLV High Viscosity, Heat Stabilized Nylon 66
Description: Polynil P240 HSLV was developed for injection molding applications, where a combination of heat aging resistance, abrasion resistance and impact strength is needed, such as chain tensio..
Deflection Temperature at 1.8 MPa (264 psi) 71.0 - 145 °C
160 - 293 °F
Average value: 102 °C Grade Count:14
Overview of materials for Acetal Copolymer, Silicone Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Silicone Filled". Each property range of values reported is minimum and maximum values..
Deflection Temperature at 1.8 MPa (264 psi) 71.0 °C
160 °F
ISO 75-1/-2
DuPont Performance Polymers Delrin® 100T BK602 Acetal Homopolymer  (Unverified Data**)
Delrin® 100T BK602 is a toughened, high viscosity acetal homopolymer grade with superior impact resistance. It is designed for highly stressed parts where outstanding toughness is required.Informa..
Deflection Temperature at 1.8 MPa (264 psi) 71.0 °C
160 °F
ISO 75-1,-2
Inno-Comp INNOPOL® CS 1-3120 B DEL 20% Talc Filled Polypropylene Homopolymer
INNOPOL® CS 1-3120 B DEL is developed for producing injection molded automotive components.All information provided by INNO-COMP.
Deflection Temperature at 1.8 MPa (264 psi) 71.0 °C

@Thickness 3.20 mm
160 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP LUBRICOMP RL004 PA 66
LNP* LUBRICOMP* RL004 is a copmpound based on Nylon 66 resin containing 20% PTFE. Added feature of this grade includes: Wear Resistant.
Deflection Temperature at 1.8 MPa (264 psi) 71.1 °C
160 °F
Unannealed; ASTM D648
Techmer ES Elastoblend® PA6/6 HI BK Nylon 66
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubricant and Impact ModifiedUl File Number: E157318Appearance: BlackProce..
Deflection Temperature at 1.8 MPa (264 psi) 71.1 °C
160 °F
ASTM D648
Techmer ES Electrafil® PS-31/EC BK Polystyrene, Electrically Conductive Carbon Black
Deflection Temperature at 1.8 MPa (264 psi) 71.1 °C
160 °F
Unannealed; ASTM D648
Techmer ES HiFill FR® PBT FR X
Availability: North AmericaForms: PelletsAdditive: Mold ReleaseFeatures: Flame RetardantProcessing Method: Injection MoldingInformation provided by TP Composites, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 71.0 °C

@Thickness 3.20 mm
160 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics NORYL PPX PPX7200 PPE+PP+PS (Europe-Africa-Middle East)
PP+PPE+PS. Improved chemical resistance and surface aesthetics in injection molded applications. NSF61-capable. UL-94 HB listed.
Deflection Temperature at 1.8 MPa (264 psi) 71.1 °C
160 °F
Unannealed; ASTM D648
Techmer ES Elastoblend® PA6/6 IM 408 HS L Nylon 66
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubricant and Impact ModifiedProcessing Method: Injection MoldingInformati..
Deflection Temperature at 1.8 MPa (264 psi) 71.0 °C

@Thickness 3.20 mm
160 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP STAT-KON RD000I PA 66
LNP* STAT-KON* RD000I is a compound based on Nylon 66 resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact.
Deflection Temperature at 1.8 MPa (264 psi) 71.0 °C
160 °F
Conditioned 4 hours @ 70°C (158°F); ASTM D648
Eastman Tenite Propionate 380A2R30015 Natural, Trsp Cellulose Acetate Propionate
Plasticizer 15%. Weight loss on heating = 0.7% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Deflection Temperature at 1.8 MPa (264 psi) 71.0 °C
160 °F
ISO 75-1/-2
DuPont Performance Polymers Delrin® 100TE NC010 Acetal (POM)  (Unverified Data**)
Toughened High Viscosity Acetal Homopolymer with Very Low Emissions Delrin 100TE NC010 (formerly DE20580) is a high viscosity toughened acetal homopolymer with very low VOC emissions. Processing met..
Deflection Temperature at 1.8 MPa (264 psi) 71.0 °C
160 °F
ISO 75-2
Denka TE-10 Transparent Resin Polymer (MABS resin) ABS
"TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a..
Deflection Temperature at 1.8 MPa (264 psi) 71.0 °C
160 °F
ISO 75-1/-2
DuPont Performance Polymers Delrin® 300TE NC010 Acetal (POM)  (Unverified Data**)
Toughened Medium-high Viscosity Acetal Homopolymer with Very Low EmissionsDelrin 300TE NC010 is a medium-high viscosity toughened acetal homopolymer with very low VOC emissions. Processing methods i..
Deflection Temperature at 1.8 MPa (264 psi) 71.0 °C
160 °F
BASF Procom® T20H S63 Polypropylene
Car heater casings.Data was collected by ISO methods and provided by BASF.
Deflection Temperature at 1.8 MPa (264 psi) 71.0 °C
160 °F
ASTM D648
Ashley Polymers Ashlene® 525LD Nylon 66
High impact Nylon 66 with good stiffness, for injection molding.Data provided by the manufacturer
Deflection Temperature at 1.8 MPa (264 psi) 71.1 °C
160 °F
ASTM D-648
Axiall 7555 Rigid PVC, Extrusion, White
Georgia Gulf 7555 is a special purpose rigid PVC extrusion compound designed for applications requiring the following properties: ToughnessDurabilityUL RatingChemical ResistanceEase of ProcessingIn..
Deflection Temperature at 1.8 MPa (264 psi) 71.1 °C
160 °F
ASTM D-648
Axiall Tuf-Stif 2804 Rigid PVC, Extrusion
Georgia Gulf Tuf-Stif 2804 is a special purpose rigid PVC profile extrusion compound designed for applications requiring the following properties: Improved toughness as compared to Tuf-StiffRigidit..
Deflection Temperature at 1.8 MPa (264 psi) 71.0 °C
160 °F
ASTM D648
A. Schulman POLYFLAM™ FPP 1006S Talc Filled Homopolymer Polypropylene
DescriptionPolyfort® FPP 1006S is a 20% talc filled homopolymer polypropylene compound formulated with an internal mold release. Information provided by A. Schulman.