Material Notes:
Type: Estane® R175A is a Shore 75A, plasticized grade thermoplastic polyurethane (TPU).Uses: Injection Molding.Information Provided by The Lubrizol Corporation
Physical Properties Metric English Comments
Specific Gravity 1.13 g/cc
1.13 g/cc
ASTM D792
Linear Mold Shrinkage 0.010 cm/cm
0.010 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 82
82
ASTM D2240
Tensile Strength, Ultimate 29.4 MPa
4270 psi
ASTM D412
Tensile Strength, Yield 4.61 MPa
668 psi
at 100% elongation; ASTM D412
8.83 MPa
1280 psi
at 300% elongation; ASTM D412
Elongation at Break 800 %
800 %
ASTM D412
Tear Strength 78.5 kN/m
448 pli
Die C; ASTM D624
Abrasion 35
35
mm<sup>3</sup> loss; ISO 4649
Compression Set 15 %

@Temperature 23.0 °C,
Time 79200 sec
15 %

@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395
45 %

@Temperature 70.0 °C,
Time 79200 sec
45 %

@Temperature 158 °F,
Time 22.0 hour
ASTM D395
Thermal Properties Metric English Comments
Vicat Softening Point 78.0 °C
172 °F
ASTM D1525